PROCESS FOR UTILIZATION OF OPEN-HEARTH SLAG SOLUTION

A process for utilization of open-hearth slag melt comprises the preparation of slag hard material and its pouring with liquid slag melt. A form is filled with dry, cooled and grinded slag material in quantity of 60-70 % by volume and filled with fusion of slag at temperature not less than 1300 °C....

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHMAT KOSTIANTYN VASYLIOVYCH, KARAKASH OLEKSANDR IVANOVYCH, YEFIMENKO YURII HEORHIIOVYCH
Format: Patent
Sprache:eng ; rus ; ukr
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A process for utilization of open-hearth slag melt comprises the preparation of slag hard material and its pouring with liquid slag melt. A form is filled with dry, cooled and grinded slag material in quantity of 60-70 % by volume and filled with fusion of slag at temperature not less than 1300 °C. Способ утилизации мартеновского шлакового расплава включает подготовку шлакового твердого материала и его заливку жидким шлаковым расплавом. Форму заполняют сухим, остывшим и дробленным, шлаковым материалом в количестве 60-70 % от объема и заливают расплавом шлака при температуре не ниже 1300 °С. Спосіб утилізації мартенівського шлакового розплаву включає підготовку шлакового твердого матеріалу і його заливку рідким шлаковим розплавом. Форму заповнюють сухим роздробленим шлаковим матеріалом, який застиг, у кількості 60-70 % від її об'єму і заливають розплавом шлаку при температурі не нижче 1300 °С.