METHOD OF FORMING OXIDE CERAMIC COATINGS ON TITANIUM AND ITS ALLOYS

The method of forming oxide-ceramic coatings on titanium and its alloys is carried out by anodic spark oxidation in solution. An aqueous solution containing both soluble Ca and P salts with concentrations of calcium hypophosphite 1-50 g/l, calcium dihydrogen phosphate 1-50 g/l is used, and the coati...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Kalinichenko Oleh Oleksandrovych, Kovalov Stanislav Viacheslavovych, Sukhyi Kostiantyn Mykhailovych, Sukhyi Mykhailo Kostiantynovych
Format: Patent
Sprache:eng ; ukr
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The method of forming oxide-ceramic coatings on titanium and its alloys is carried out by anodic spark oxidation in solution. An aqueous solution containing both soluble Ca and P salts with concentrations of calcium hypophosphite 1-50 g/l, calcium dihydrogen phosphate 1-50 g/l is used, and the coating is applied in a galvanostatic mode with a current density of 1000-3000 A/m2, solution temperature 20-25 °C, for 5-50 minutes. Спосіб формування оксидно-керамічних покриттів на титані і його сплавах здійснюють методом анодно-іскрового оксидування в розчині. При цьому використовують водний розчин, що містить одночасно розчинні солі Са та Р, з концентраціями гіпофосфіту кальцію 1-50 г/л, дигідрофосфату кальцію 1-50 г/л, та покриття наносять у гальваностатичному режимі з густиною струму 1000-3000 А/м2, температурою розчину 20-25 °C, протягом 5-50 хв.