METHOD OF COMBINED MODIFICATION OF THE SURFACE OF THE PART

The method of combined modification of the surface of a part includes boring the surface of the part and radiation treatment of the surface after boring. Boroning is carried out in a furnace in an environment of boron-containing substances at a temperature of 850 °C with a holding time of 7 hours, a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Lysenko Oleksandr Borysovych, Cherneta Oleh Heorhiiovych, Averyanov Volodymyr Serhiiovych, Sasov Oleksandr Oleksandrovych, Sereda Borys Petrovych, Kubich Vadym Ivanovych
Format: Patent
Sprache:eng ; ukr
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Lysenko Oleksandr Borysovych
Cherneta Oleh Heorhiiovych
Averyanov Volodymyr Serhiiovych
Sasov Oleksandr Oleksandrovych
Sereda Borys Petrovych
Kubich Vadym Ivanovych
description The method of combined modification of the surface of a part includes boring the surface of the part and radiation treatment of the surface after boring. Boroning is carried out in a furnace in an environment of boron-containing substances at a temperature of 850 °C with a holding time of 7 hours, and radiation treatment is carried out with a pulsed laser at an accumulation energy E = 28 kJ with a laser beam diameter of 8 mm, with an overlap of treatment zones of 15 % and a laser pulse duration of 1×10-3-2×10-3 s and a distance to the target of 70 mm. Спосіб комбінованої модифікації поверхні деталі включає борування поверхні деталі і променеву обробку поверхні після борування. Борування здійснюють в печі в середовищі боровмісних речовин при температурі 850 °C з витримкою 7 годин, а променеву обробку здійснюють імпульсним лазером при енергії накопичення Е=28 кДж діаметром лазерного пучка 8 мм, з коефіцієнтом перекриття зон обробки 15 % та тривалості імпульсу лазерного випромінювання 1 10-3-2210-3 с і з відстанню до мішені 70 мм.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_UA151554UU</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>UA151554UU</sourcerecordid><originalsourceid>FETCH-epo_espacenet_UA151554UU3</originalsourceid><addsrcrecordid>eNrjZLDydQ3x8HdR8HdTcPb3dfL0c3VR8PV38XTzdHYM8fT3A0mEeLgqBIcGuTk6u8K4AY5BITwMrGmJOcWpvFCam0HezTXE2UM3tSA_PrW4IDE5NS-1JD7U0dDU0NTUJDTUmLAKAOacKBw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF COMBINED MODIFICATION OF THE SURFACE OF THE PART</title><source>esp@cenet</source><creator>Lysenko Oleksandr Borysovych ; Cherneta Oleh Heorhiiovych ; Averyanov Volodymyr Serhiiovych ; Sasov Oleksandr Oleksandrovych ; Sereda Borys Petrovych ; Kubich Vadym Ivanovych</creator><creatorcontrib>Lysenko Oleksandr Borysovych ; Cherneta Oleh Heorhiiovych ; Averyanov Volodymyr Serhiiovych ; Sasov Oleksandr Oleksandrovych ; Sereda Borys Petrovych ; Kubich Vadym Ivanovych</creatorcontrib><description>The method of combined modification of the surface of a part includes boring the surface of the part and radiation treatment of the surface after boring. Boroning is carried out in a furnace in an environment of boron-containing substances at a temperature of 850 °C with a holding time of 7 hours, and radiation treatment is carried out with a pulsed laser at an accumulation energy E = 28 kJ with a laser beam diameter of 8 mm, with an overlap of treatment zones of 15 % and a laser pulse duration of 1×10-3-2×10-3 s and a distance to the target of 70 mm. Спосіб комбінованої модифікації поверхні деталі включає борування поверхні деталі і променеву обробку поверхні після борування. Борування здійснюють в печі в середовищі боровмісних речовин при температурі 850 °C з витримкою 7 годин, а променеву обробку здійснюють імпульсним лазером при енергії накопичення Е=28 кДж діаметром лазерного пучка 8 мм, з коефіцієнтом перекриття зон обробки 15 % та тривалості імпульсу лазерного випромінювання 1 10-3-2210-3 с і з відстанню до мішені 70 мм.</description><language>eng ; ukr</language><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220810&amp;DB=EPODOC&amp;CC=UA&amp;NR=151554U$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220810&amp;DB=EPODOC&amp;CC=UA&amp;NR=151554U$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Lysenko Oleksandr Borysovych</creatorcontrib><creatorcontrib>Cherneta Oleh Heorhiiovych</creatorcontrib><creatorcontrib>Averyanov Volodymyr Serhiiovych</creatorcontrib><creatorcontrib>Sasov Oleksandr Oleksandrovych</creatorcontrib><creatorcontrib>Sereda Borys Petrovych</creatorcontrib><creatorcontrib>Kubich Vadym Ivanovych</creatorcontrib><title>METHOD OF COMBINED MODIFICATION OF THE SURFACE OF THE PART</title><description>The method of combined modification of the surface of a part includes boring the surface of the part and radiation treatment of the surface after boring. Boroning is carried out in a furnace in an environment of boron-containing substances at a temperature of 850 °C with a holding time of 7 hours, and radiation treatment is carried out with a pulsed laser at an accumulation energy E = 28 kJ with a laser beam diameter of 8 mm, with an overlap of treatment zones of 15 % and a laser pulse duration of 1×10-3-2×10-3 s and a distance to the target of 70 mm. Спосіб комбінованої модифікації поверхні деталі включає борування поверхні деталі і променеву обробку поверхні після борування. Борування здійснюють в печі в середовищі боровмісних речовин при температурі 850 °C з витримкою 7 годин, а променеву обробку здійснюють імпульсним лазером при енергії накопичення Е=28 кДж діаметром лазерного пучка 8 мм, з коефіцієнтом перекриття зон обробки 15 % та тривалості імпульсу лазерного випромінювання 1 10-3-2210-3 с і з відстанню до мішені 70 мм.</description><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDydQ3x8HdR8HdTcPb3dfL0c3VR8PV38XTzdHYM8fT3A0mEeLgqBIcGuTk6u8K4AY5BITwMrGmJOcWpvFCam0HezTXE2UM3tSA_PrW4IDE5NS-1JD7U0dDU0NTUJDTUmLAKAOacKBw</recordid><startdate>20220810</startdate><enddate>20220810</enddate><creator>Lysenko Oleksandr Borysovych</creator><creator>Cherneta Oleh Heorhiiovych</creator><creator>Averyanov Volodymyr Serhiiovych</creator><creator>Sasov Oleksandr Oleksandrovych</creator><creator>Sereda Borys Petrovych</creator><creator>Kubich Vadym Ivanovych</creator><scope>EVB</scope></search><sort><creationdate>20220810</creationdate><title>METHOD OF COMBINED MODIFICATION OF THE SURFACE OF THE PART</title><author>Lysenko Oleksandr Borysovych ; Cherneta Oleh Heorhiiovych ; Averyanov Volodymyr Serhiiovych ; Sasov Oleksandr Oleksandrovych ; Sereda Borys Petrovych ; Kubich Vadym Ivanovych</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_UA151554UU3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; ukr</language><creationdate>2022</creationdate><toplevel>online_resources</toplevel><creatorcontrib>Lysenko Oleksandr Borysovych</creatorcontrib><creatorcontrib>Cherneta Oleh Heorhiiovych</creatorcontrib><creatorcontrib>Averyanov Volodymyr Serhiiovych</creatorcontrib><creatorcontrib>Sasov Oleksandr Oleksandrovych</creatorcontrib><creatorcontrib>Sereda Borys Petrovych</creatorcontrib><creatorcontrib>Kubich Vadym Ivanovych</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Lysenko Oleksandr Borysovych</au><au>Cherneta Oleh Heorhiiovych</au><au>Averyanov Volodymyr Serhiiovych</au><au>Sasov Oleksandr Oleksandrovych</au><au>Sereda Borys Petrovych</au><au>Kubich Vadym Ivanovych</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF COMBINED MODIFICATION OF THE SURFACE OF THE PART</title><date>2022-08-10</date><risdate>2022</risdate><abstract>The method of combined modification of the surface of a part includes boring the surface of the part and radiation treatment of the surface after boring. Boroning is carried out in a furnace in an environment of boron-containing substances at a temperature of 850 °C with a holding time of 7 hours, and radiation treatment is carried out with a pulsed laser at an accumulation energy E = 28 kJ with a laser beam diameter of 8 mm, with an overlap of treatment zones of 15 % and a laser pulse duration of 1×10-3-2×10-3 s and a distance to the target of 70 mm. Спосіб комбінованої модифікації поверхні деталі включає борування поверхні деталі і променеву обробку поверхні після борування. Борування здійснюють в печі в середовищі боровмісних речовин при температурі 850 °C з витримкою 7 годин, а променеву обробку здійснюють імпульсним лазером при енергії накопичення Е=28 кДж діаметром лазерного пучка 8 мм, з коефіцієнтом перекриття зон обробки 15 % та тривалості імпульсу лазерного випромінювання 1 10-3-2210-3 с і з відстанню до мішені 70 мм.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; ukr
recordid cdi_epo_espacenet_UA151554UU
source esp@cenet
title METHOD OF COMBINED MODIFICATION OF THE SURFACE OF THE PART
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-18T07%3A00%3A47IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Lysenko%20Oleksandr%20Borysovych&rft.date=2022-08-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUA151554UU%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true