METHOD OF COMBINED MODIFICATION OF THE SURFACE OF THE PART

The method of combined modification of the surface of a part includes boring the surface of the part and radiation treatment of the surface after boring. Boroning is carried out in a furnace in an environment of boron-containing substances at a temperature of 850 °C with a holding time of 7 hours, a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Lysenko Oleksandr Borysovych, Cherneta Oleh Heorhiiovych, Averyanov Volodymyr Serhiiovych, Sasov Oleksandr Oleksandrovych, Sereda Borys Petrovych, Kubich Vadym Ivanovych
Format: Patent
Sprache:eng ; ukr
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The method of combined modification of the surface of a part includes boring the surface of the part and radiation treatment of the surface after boring. Boroning is carried out in a furnace in an environment of boron-containing substances at a temperature of 850 °C with a holding time of 7 hours, and radiation treatment is carried out with a pulsed laser at an accumulation energy E = 28 kJ with a laser beam diameter of 8 mm, with an overlap of treatment zones of 15 % and a laser pulse duration of 1×10-3-2×10-3 s and a distance to the target of 70 mm. Спосіб комбінованої модифікації поверхні деталі включає борування поверхні деталі і променеву обробку поверхні після борування. Борування здійснюють в печі в середовищі боровмісних речовин при температурі 850 °C з витримкою 7 годин, а променеву обробку здійснюють імпульсним лазером при енергії накопичення Е=28 кДж діаметром лазерного пучка 8 мм, з коефіцієнтом перекриття зон обробки 15 % та тривалості імпульсу лазерного випромінювання 1 10-3-2210-3 с і з відстанню до мішені 70 мм.