METHOD FOR THE APPLICATION OF PROTECTIVE CHROMIFEROUS COATINS ON STAINLESS STEEL

A method for forming chromiferous oxide coatings on stainless steel involves oxidation in aqueous electrolyte. The deposition process is carried out for 30-90 minutes using pulse current of square form at current density of 90-130 A/dm2, pulse duration of 0.25-1 s, pause length of 0.25-1 s. Спосіб ф...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Shtefan Viktoriia Volodymyrivna, Balamut Nataliia Serhiivna, Kanunnikova Nadiia Oleksandrivna
Format: Patent
Sprache:eng ; ukr
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A method for forming chromiferous oxide coatings on stainless steel involves oxidation in aqueous electrolyte. The deposition process is carried out for 30-90 minutes using pulse current of square form at current density of 90-130 A/dm2, pulse duration of 0.25-1 s, pause length of 0.25-1 s. Спосіб формування хромвмісних оксидних покриттів на нержавіючу сталь, що включає оксидування у водному електроліті, згідно з корисною моделлю процес осадження проводять з використанням імпульсного струму прямокутної форми при густині струму 90-130 А/дм2, тривалості імпульсу 0,25-1 с, тривалості паузи 0,25-1 с впродовж 30-90 хвилин.