method for producing steel melt containing up to 30 % of manganese
The invention relates to a method for producing a steel melt containing up to 30 % of Mn, which additionally may comprise up to 5 % Si, up to 1.5 % C, up to 22 % Al, up to 25 % Cr, up to 30 % Ni, and up to 5 % each of Ti, V, NB, Cu, Sn, Zr, Mo, and W, and up to 1 % each of N and P, with the remainde...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; rus ; ukr |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a method for producing a steel melt containing up to 30 % of Mn, which additionally may comprise up to 5 % Si, up to 1.5 % C, up to 22 % Al, up to 25 % Cr, up to 30 % Ni, and up to 5 % each of Ti, V, NB, Cu, Sn, Zr, Mo, and W, and up to 1 % each of N and P, with the remainder being iron and unavoidable steel companion elements.
Винахід стосується способу одержання розплаву сталі із вмістом марганцю до 30 мас. %, в якому додатково можуть міститися, мас. %: до 5 Si, до 1,5 С, до 22 Al, до 25 Сr, до 30 Ni, а також до 5 Ті, V, Nb, Cu, Sn, Zr, Mo, W кожного, а також до 1 N і Р кожного, решта - залізо та неминучі домішки при виплавці сталі.[Изобретение относится к способу получения расплава стали с содержанием марганца до 30 мас. %, в котором дополнительно могут содержаться, масс. %: до 5 Si, до 1,5 С, до 22 Al, до 25 Cr, до 30 Ni, а также до 5 Ti, V, Nb, Cu, Sn, Zr, Mo, W каждого, а также до 1 N и Р каждого, остальное - железо и неизбежные примеси при выплавке стали. |
---|