method for forming a catalytically active coatings on titanium alloys

A method for forming a catalytically active coatings on titanium alloys by micro-arc oxidation in an electrolyte containing cerium sulfate and zirconium sulfate. The process is carried out in galvanostatic mode at a current density of 5-20 A/dm2 for 30-60 minutes in the electrolyte, which additional...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Shtefan Viktoriia Volodymyrivna, Smyrnova Oleksandra Yuriivna
Format: Patent
Sprache:eng ; rus ; ukr
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A method for forming a catalytically active coatings on titanium alloys by micro-arc oxidation in an electrolyte containing cerium sulfate and zirconium sulfate. The process is carried out in galvanostatic mode at a current density of 5-20 A/dm2 for 30-60 minutes in the electrolyte, which additionally contains sulfuric acid and copper sulfate. Способ формирования каталитически активных покрытий на титановых сплавах методом микродугового оксидирования в электролите, содержащем сульфат церия и сульфат циркония. Процесс проводят в гальваностатическом режиме при плотности тока 5-20 А/дм2 в течение 30-60 минут в электролите, который дополнительно содержит серную кислоту и сульфат меди. Спосіб формування каталітично-активних покриттів на титанових сплавах методом мікродугового оксидування в електроліті, що містить сульфат церію та сульфат цирконію. Процес проводять у гальваностатичному режимі при густині струму 5-20 А/дм2 протягом 30-60 хвилин в електроліті, що додатково містить сульфатну кислоту та сульфат міді.