Provided is a method for producing an ultra-low carbon steel product in which, even if bubbles are captured in a solidified shell, occurrence of blister defects can be suppressed in a hot rolling step and subsequent steps.A method for producing an ultra-low carbon steel product having a carbon conce...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | chi |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Provided is a method for producing an ultra-low carbon steel product in which, even if bubbles are captured in a solidified shell, occurrence of blister defects can be suppressed in a hot rolling step and subsequent steps.A method for producing an ultra-low carbon steel product having a carbon concentration of 0.005% by mass or less includes, at least, a step of adjusting a carbon concentration of molten iron to obtain molten steel, a step of casting the molten steel into a slab, and a step of hot rolling the slab to obtain a hot-rolled steel sheet, in which the method further includes a width reduction step of performing width reduction on the slab with a reduction amount which is predetermined in accordance with the slab width in a direction orthogonal to the rolling direction of the slab. |
---|