Glass and method for manufacturing glass

Glass contains, in mol percentage on an oxide basis, SiO2: 35% to 60%, B2O3: 0.8% to 8%, Al2O3: 6% to 21%, and MgO: 17% to 44%. Additionally, (MgO/Al2O3) ≥ 1 is satisfied, a measured Madelung constant m calculated by an expression (1A) is equal to or larger than 1.05, and a thermal expansion factor...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NAGANO, MIKIO, KADO, RIKIYA, TAMAI, KIYOSHI, INABA, SEIJI, KOBAYASHI, YUHA
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Glass contains, in mol percentage on an oxide basis, SiO2: 35% to 60%, B2O3: 0.8% to 8%, Al2O3: 6% to 21%, and MgO: 17% to 44%. Additionally, (MgO/Al2O3) ≥ 1 is satisfied, a measured Madelung constant m calculated by an expression (1A) is equal to or larger than 1.05, and a thermal expansion factor as a ratio of a measured value [alpha] of a linear thermal expansion coefficient to a calculated value [alpha]cal of a linear thermal expansion coefficient calculated from composition is equal to or smaller than 0.7. Herein, E is a measured value of a Young's modulus of the glass, Vp is an average atomic packing factor of the glass, and Gt is average bond dissociation energy of the glass.