METHOD TO PRODUCE HIGH-TEMPERATURE SUPERCONDUCTING MATERIAL BiSrCaCuO+δ

FIELD: high-temperature superconducting materials synthesis. SUBSTANCE: charge of stoichiometric composition corresponding to composition of material BiSrCaCuO+δ is prepared and annealed, melted and hardened in the open air and then it is subjected to thermal treatment under temperature of 840 - 845...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Shnejder A.G, Seljavko A.I
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: high-temperature superconducting materials synthesis. SUBSTANCE: charge of stoichiometric composition corresponding to composition of material BiSrCaCuO+δ is prepared and annealed, melted and hardened in the open air and then it is subjected to thermal treatment under temperature of 840 - 845 C at least for 10 hours. After that material has share of BI-2212 phase equal to 70 - 90 %. EFFECT: simplified process. Использование: в технологии синтеза высокотемпературных сверхпроводящих материалов. Сущность изобретения: готовят шихту стехиометрического состава, соответственно составу материалаBiSrCaCuO+δотжигают ее, расплавляют и закаливают на воздухе, после чего проводят термообработку при 840 - 845С не менее 10 ч. Свойства материала: процентное содержание фазы Bi - 2212 составляет 70 - 90%.