METHOD OF THERMOSTABLE FIBER PRODUCING

FIELD: composition thermostable materials. SUBSTANCE: method involves the use of synthesis of poly-(o-aminophenylenenaphthoyleneamide) by condensation in the medium of N-methylpyrrolidone, and 10-17% solution of polymer is obtained showing intrinsic viscosity value 1.2-1.9 dl/g followed by forming i...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Tikhonov I.V, Ponomarev I.I, Frenkel' G.G, Terenin V.I
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: composition thermostable materials. SUBSTANCE: method involves the use of synthesis of poly-(o-aminophenylenenaphthoyleneamide) by condensation in the medium of N-methylpyrrolidone, and 10-17% solution of polymer is obtained showing intrinsic viscosity value 1.2-1.9 dl/g followed by forming in settler bath containing N-methylpyrrolidone. Then plasticizing stretching, washing and drying were carried out. Then fiber is treated at 370-390 C for 1.5-2 hr in argon atmosphere under pressure 10-15 mm mercury column followed by thermic stretching. EFFECT: improved method of fiber producing. Использование: композиционные термостойкие материалы, применяемые в технических целях. Сущность изобретения: синтезируют поли-(0-аминофениленнафтоиленамид) поликонденсацией в среде N-метиллирролидона, получая непосредственно 10 - 17%-ный раствор с характеристической вязкостью полимера 1,2 - 1,9 дл/г. Формуют в осадительную ванну, содержащую N-метилпирролидон. Осуществляют пластификационную вытяжку, промывку, сушку. Затем волокно обрабатывают при 370 - 390С 1,5 - 2 ч в среде аргона или при давлении 10 - 15 мм рт.ст. и термовытягивают.