METHOD FOR EXPLOITATION OF INHOMOGENEOUS OIL POOL
FIELD: oil production. SUBSTANCE: 0.01 - 0.05 per cent solution of polyacrylamide, then 0.01 - 1.5 per cent solution of calcium chloride and then clay suspension are pumped in the pool subsequently. This cycle is repeated several times. EFFECT: higher productivity. 1 tbl Изобретение относится к нефт...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: oil production. SUBSTANCE: 0.01 - 0.05 per cent solution of polyacrylamide, then 0.01 - 1.5 per cent solution of calcium chloride and then clay suspension are pumped in the pool subsequently. This cycle is repeated several times. EFFECT: higher productivity. 1 tbl
Изобретение относится к нефтедобывающей промышленности, к способам разработки неоднородного нефтяного пласта. Цель изобретения - повышение эффективности способа за счет более полной изоляции обводнившегося пропластка путем повышения осаждения глинистых частиц и устойчивости к размыву изолирующего материала. В пласт закачивается 0,01-0,05%-ный раствор частично гидролизованного полиакриламида, затем 0,01-1,5%-ный раствор хлористого кальция и затем глинистая суспензия. Этот цикл повторяют несколько раз. При использовании данного способа в 1,5 раза увеличивается полнота осаждения глинистых частиц в результате взаимодействия с хлористым кальцием, а также в 2,7 раза повышается прочность осадка. Это позволяет увеличить длительность изоляционного эффекта, что сокращает количество обработок скважин изолирующим материалом и экономию химреагентов. 2 табл. |
---|