METHOD OF FLUXLESS SOLDERING OF ALUMINIUM STRUCTURES

FIELD: mechanical engineering; fluxless soldering of large-size aluminium structures, mainly plate-and-rib heat exchangers. SUBSTANCE: article to be soldered is assembled, and silumin-based solder is applied to zone of soldering. Assembled article is placed into furnace chamber. The preliminary heat...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Baranov N.S, Kurtashin V.E, Storchaj E.I, Gustov V.F, Tarasenko L.S, Sokolova A.V, Filin N.V
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Baranov N.S
Kurtashin V.E
Storchaj E.I
Gustov V.F
Tarasenko L.S
Sokolova A.V
Filin N.V
description FIELD: mechanical engineering; fluxless soldering of large-size aluminium structures, mainly plate-and-rib heat exchangers. SUBSTANCE: article to be soldered is assembled, and silumin-based solder is applied to zone of soldering. Assembled article is placed into furnace chamber. The preliminary heating and repeated evacuation of chamber is carried out with filling of chamber with inert gas after each evacuation. Subsequent heating from temperature of 140-170 C to soldering temperature is provided by turbulent flow of inert gas circulating in chamber. Dew point of inert gas does not exceed 90 C. Oxygen content in inert gas does not exceed 5*10vol.%. Gas is delivered into chamber article inner space through solid nonflashed getter. Circulation of gas and gas temperature rise are provided by aerodynamic heaters. Turbulent flow of inert gas of indicated cleanness provides high speed and uniform heating of article without oxidation of soldered surface dangerous for soldering. EFFECT: improved reliability of soldering over entire volume of article without erosion of thin-walled members, reduced time of diffusion and solution interaction between structure material and solder. 2 cl Изобретение относится к пайке, в частности к бесфлюсовой пайке крупногабаритных алюминиевых конструкций, преимущественно пластинчато-ребристых теплообменников. Цель изобретения - повышение качества крупногабаритных паяных изделий путем сокращения времени диффузионного и растворного взаимодействия материала конструкции с припоем. Паяемое изделие собирают с размещением в зоне пайки припоя на основе силумина. Загружают изделие в камеру печи. Производят предварительный нагрев, многократное вакуумирование камеры с последующим заполнением инертным газом после каждого вакуумирования. Последующий нагрев от температуры 140 - 170C до температуры пайки производят турбулентным потоком циркулирующего в камере инертного газа с точкой росы не выше -90C с содержанием кислорода не более 5*10об.%, подаваемого во внутреннюю полость изделия через твердый нераспыляемый геттер. Циркуляция газа и повышение его температуры обеспечивается аэродинамическими нагревателями. Турбулентный поток инертного газа указанной чистоты обеспечивает высокую скорость и равномерность нагрева изделия без опасного для пайки окисления паяемых поверхностей. Высокая скорость нагрева обеспечивает надежность пайки по всему объему изделия без эрозии тонкостенных элементов. 1 з.п. ф-лы.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_SU1543711A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>SU1543711A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_SU1543711A13</originalsourceid><addsrcrecordid>eNrjZDDxdQ3x8HdR8HdTcPMJjfBxDQ5WCPb3cXEN8vRzB4k6-oT6evp5hvoqBIcEhTqHhAa5BvMwsKYl5hSn8kJpbgYFN9cQZw_d1IL8-NTigsTk1LzUkvjgUENTE2NzQ0NHQ2MilAAAoAQncg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF FLUXLESS SOLDERING OF ALUMINIUM STRUCTURES</title><source>esp@cenet</source><creator>Baranov N.S ; Kurtashin V.E ; Storchaj E.I ; Gustov V.F ; Tarasenko L.S ; Sokolova A.V ; Filin N.V</creator><creatorcontrib>Baranov N.S ; Kurtashin V.E ; Storchaj E.I ; Gustov V.F ; Tarasenko L.S ; Sokolova A.V ; Filin N.V</creatorcontrib><description>FIELD: mechanical engineering; fluxless soldering of large-size aluminium structures, mainly plate-and-rib heat exchangers. SUBSTANCE: article to be soldered is assembled, and silumin-based solder is applied to zone of soldering. Assembled article is placed into furnace chamber. The preliminary heating and repeated evacuation of chamber is carried out with filling of chamber with inert gas after each evacuation. Subsequent heating from temperature of 140-170 C to soldering temperature is provided by turbulent flow of inert gas circulating in chamber. Dew point of inert gas does not exceed 90 C. Oxygen content in inert gas does not exceed 5*10vol.%. Gas is delivered into chamber article inner space through solid nonflashed getter. Circulation of gas and gas temperature rise are provided by aerodynamic heaters. Turbulent flow of inert gas of indicated cleanness provides high speed and uniform heating of article without oxidation of soldered surface dangerous for soldering. EFFECT: improved reliability of soldering over entire volume of article without erosion of thin-walled members, reduced time of diffusion and solution interaction between structure material and solder. 2 cl Изобретение относится к пайке, в частности к бесфлюсовой пайке крупногабаритных алюминиевых конструкций, преимущественно пластинчато-ребристых теплообменников. Цель изобретения - повышение качества крупногабаритных паяных изделий путем сокращения времени диффузионного и растворного взаимодействия материала конструкции с припоем. Паяемое изделие собирают с размещением в зоне пайки припоя на основе силумина. Загружают изделие в камеру печи. Производят предварительный нагрев, многократное вакуумирование камеры с последующим заполнением инертным газом после каждого вакуумирования. Последующий нагрев от температуры 140 - 170C до температуры пайки производят турбулентным потоком циркулирующего в камере инертного газа с точкой росы не выше -90C с содержанием кислорода не более 5*10об.%, подаваемого во внутреннюю полость изделия через твердый нераспыляемый геттер. Циркуляция газа и повышение его температуры обеспечивается аэродинамическими нагревателями. Турбулентный поток инертного газа указанной чистоты обеспечивает высокую скорость и равномерность нагрева изделия без опасного для пайки окисления паяемых поверхностей. Высокая скорость нагрева обеспечивает надежность пайки по всему объему изделия без эрозии тонкостенных элементов. 1 з.п. ф-лы.</description><language>eng ; rus</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>1997</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19970227&amp;DB=EPODOC&amp;CC=SU&amp;NR=1543711A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19970227&amp;DB=EPODOC&amp;CC=SU&amp;NR=1543711A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Baranov N.S</creatorcontrib><creatorcontrib>Kurtashin V.E</creatorcontrib><creatorcontrib>Storchaj E.I</creatorcontrib><creatorcontrib>Gustov V.F</creatorcontrib><creatorcontrib>Tarasenko L.S</creatorcontrib><creatorcontrib>Sokolova A.V</creatorcontrib><creatorcontrib>Filin N.V</creatorcontrib><title>METHOD OF FLUXLESS SOLDERING OF ALUMINIUM STRUCTURES</title><description>FIELD: mechanical engineering; fluxless soldering of large-size aluminium structures, mainly plate-and-rib heat exchangers. SUBSTANCE: article to be soldered is assembled, and silumin-based solder is applied to zone of soldering. Assembled article is placed into furnace chamber. The preliminary heating and repeated evacuation of chamber is carried out with filling of chamber with inert gas after each evacuation. Subsequent heating from temperature of 140-170 C to soldering temperature is provided by turbulent flow of inert gas circulating in chamber. Dew point of inert gas does not exceed 90 C. Oxygen content in inert gas does not exceed 5*10vol.%. Gas is delivered into chamber article inner space through solid nonflashed getter. Circulation of gas and gas temperature rise are provided by aerodynamic heaters. Turbulent flow of inert gas of indicated cleanness provides high speed and uniform heating of article without oxidation of soldered surface dangerous for soldering. EFFECT: improved reliability of soldering over entire volume of article without erosion of thin-walled members, reduced time of diffusion and solution interaction between structure material and solder. 2 cl Изобретение относится к пайке, в частности к бесфлюсовой пайке крупногабаритных алюминиевых конструкций, преимущественно пластинчато-ребристых теплообменников. Цель изобретения - повышение качества крупногабаритных паяных изделий путем сокращения времени диффузионного и растворного взаимодействия материала конструкции с припоем. Паяемое изделие собирают с размещением в зоне пайки припоя на основе силумина. Загружают изделие в камеру печи. Производят предварительный нагрев, многократное вакуумирование камеры с последующим заполнением инертным газом после каждого вакуумирования. Последующий нагрев от температуры 140 - 170C до температуры пайки производят турбулентным потоком циркулирующего в камере инертного газа с точкой росы не выше -90C с содержанием кислорода не более 5*10об.%, подаваемого во внутреннюю полость изделия через твердый нераспыляемый геттер. Циркуляция газа и повышение его температуры обеспечивается аэродинамическими нагревателями. Турбулентный поток инертного газа указанной чистоты обеспечивает высокую скорость и равномерность нагрева изделия без опасного для пайки окисления паяемых поверхностей. Высокая скорость нагрева обеспечивает надежность пайки по всему объему изделия без эрозии тонкостенных элементов. 1 з.п. ф-лы.</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1997</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDxdQ3x8HdR8HdTcPMJjfBxDQ5WCPb3cXEN8vRzB4k6-oT6evp5hvoqBIcEhTqHhAa5BvMwsKYl5hSn8kJpbgYFN9cQZw_d1IL8-NTigsTk1LzUkvjgUENTE2NzQ0NHQ2MilAAAoAQncg</recordid><startdate>19970227</startdate><enddate>19970227</enddate><creator>Baranov N.S</creator><creator>Kurtashin V.E</creator><creator>Storchaj E.I</creator><creator>Gustov V.F</creator><creator>Tarasenko L.S</creator><creator>Sokolova A.V</creator><creator>Filin N.V</creator><scope>EVB</scope></search><sort><creationdate>19970227</creationdate><title>METHOD OF FLUXLESS SOLDERING OF ALUMINIUM STRUCTURES</title><author>Baranov N.S ; Kurtashin V.E ; Storchaj E.I ; Gustov V.F ; Tarasenko L.S ; Sokolova A.V ; Filin N.V</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_SU1543711A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>1997</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>Baranov N.S</creatorcontrib><creatorcontrib>Kurtashin V.E</creatorcontrib><creatorcontrib>Storchaj E.I</creatorcontrib><creatorcontrib>Gustov V.F</creatorcontrib><creatorcontrib>Tarasenko L.S</creatorcontrib><creatorcontrib>Sokolova A.V</creatorcontrib><creatorcontrib>Filin N.V</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Baranov N.S</au><au>Kurtashin V.E</au><au>Storchaj E.I</au><au>Gustov V.F</au><au>Tarasenko L.S</au><au>Sokolova A.V</au><au>Filin N.V</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF FLUXLESS SOLDERING OF ALUMINIUM STRUCTURES</title><date>1997-02-27</date><risdate>1997</risdate><abstract>FIELD: mechanical engineering; fluxless soldering of large-size aluminium structures, mainly plate-and-rib heat exchangers. SUBSTANCE: article to be soldered is assembled, and silumin-based solder is applied to zone of soldering. Assembled article is placed into furnace chamber. The preliminary heating and repeated evacuation of chamber is carried out with filling of chamber with inert gas after each evacuation. Subsequent heating from temperature of 140-170 C to soldering temperature is provided by turbulent flow of inert gas circulating in chamber. Dew point of inert gas does not exceed 90 C. Oxygen content in inert gas does not exceed 5*10vol.%. Gas is delivered into chamber article inner space through solid nonflashed getter. Circulation of gas and gas temperature rise are provided by aerodynamic heaters. Turbulent flow of inert gas of indicated cleanness provides high speed and uniform heating of article without oxidation of soldered surface dangerous for soldering. EFFECT: improved reliability of soldering over entire volume of article without erosion of thin-walled members, reduced time of diffusion and solution interaction between structure material and solder. 2 cl Изобретение относится к пайке, в частности к бесфлюсовой пайке крупногабаритных алюминиевых конструкций, преимущественно пластинчато-ребристых теплообменников. Цель изобретения - повышение качества крупногабаритных паяных изделий путем сокращения времени диффузионного и растворного взаимодействия материала конструкции с припоем. Паяемое изделие собирают с размещением в зоне пайки припоя на основе силумина. Загружают изделие в камеру печи. Производят предварительный нагрев, многократное вакуумирование камеры с последующим заполнением инертным газом после каждого вакуумирования. Последующий нагрев от температуры 140 - 170C до температуры пайки производят турбулентным потоком циркулирующего в камере инертного газа с точкой росы не выше -90C с содержанием кислорода не более 5*10об.%, подаваемого во внутреннюю полость изделия через твердый нераспыляемый геттер. Циркуляция газа и повышение его температуры обеспечивается аэродинамическими нагревателями. Турбулентный поток инертного газа указанной чистоты обеспечивает высокую скорость и равномерность нагрева изделия без опасного для пайки окисления паяемых поверхностей. Высокая скорость нагрева обеспечивает надежность пайки по всему объему изделия без эрозии тонкостенных элементов. 1 з.п. ф-лы.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_SU1543711A1
source esp@cenet
subjects CLADDING OR PLATING BY SOLDERING OR WELDING
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title METHOD OF FLUXLESS SOLDERING OF ALUMINIUM STRUCTURES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-30T15%3A30%3A36IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Baranov%20N.S&rft.date=1997-02-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ESU1543711A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true