METHOD OF POLYAMIDOIMIDES SYNTHESIS
FIELD: chemical technology. SUBSTANCE: method involves interaction of trimellite anhydride, aromatic primary diamine and ε-caprolactam at molar ratio 1: (0.8-1): (0.2-1.2), respectively, in the presence of tri-(2-hydroxyethyl)isocyanourate at concentration 0.05-0.3 mole per 1 mole trimellite anhydri...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: chemical technology. SUBSTANCE: method involves interaction of trimellite anhydride, aromatic primary diamine and ε-caprolactam at molar ratio 1: (0.8-1): (0.2-1.2), respectively, in the presence of tri-(2-hydroxyethyl)isocyanourate at concentration 0.05-0.3 mole per 1 mole trimellite anhydride. Condensation is carried out in the medium of organic solvent at 200-220 C in the presence of catalyst up to preparing the resin with softening point 85-135 C by method "ring-and-ball". EFFECT: polyamidoimides prepared shows improved technological properties. 1 tbl
Изобретение относится к области получения полиамидоимидов, которые могут найти применение в производстве термостойких электроизоляционных смол, пленок и покрытий, в частности для эмалирования проволоки. Изобретение позволяет получить полиамидоимиды с улучшенными технологическими характеристиками путем взаимодействия тримеллитового ангидрида, ароматического первичного диамина и ε -капролактама в молярном соотношении 1 : (0,8 - 1) : (0,2 - 1,2) соответственно в присутствии три-(2-оксиэтил-изоцианурата в количестве 0,05 - 0,3 моль на 1 моль тримеллитового ангидрида и поликонденсацию проводят в среде органического растворителя при 200 - 220°С в присутствии катализатора до получения смолы с температурой размягчения по методу "кольцо и шар" 85 - 135°С. 1 табл. |
---|