LOW DEPOSITION RATES FOR FLOWABLE PECVD

PECVD methods for depositing a film at a low deposition rate comprising intermittent activation of the plasma are disclosed. The flowable film can be deposited using at least a polysilane precursor and a plasma gas. The deposition rate of the disclosed processes may be less than 500 Å/min.

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MANNA, Pramit, MALLICK, Abhijit Basu, JIANG, Shishi
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PECVD methods for depositing a film at a low deposition rate comprising intermittent activation of the plasma are disclosed. The flowable film can be deposited using at least a polysilane precursor and a plasma gas. The deposition rate of the disclosed processes may be less than 500 Å/min.