METHOD OF MAGNESIUM SILICIDE PRODUCING

FIELD: chemical technology, inorganic chemistry. SUBSTANCE: method involves the preparing mixture that consists of magnesium, silicon, silicon oxide and/or magnesium perchlorate, thermic working of mixture at "CBC" regime under inert gas pressure, mainly argon, 0.5-2.0 MPa at the following...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BOROVINSKAJA I.P, VERSHINNIKOV V.I
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: chemical technology, inorganic chemistry. SUBSTANCE: method involves the preparing mixture that consists of magnesium, silicon, silicon oxide and/or magnesium perchlorate, thermic working of mixture at "CBC" regime under inert gas pressure, mainly argon, 0.5-2.0 MPa at the following ratio of components, wt.-%: magnesium 60-63; silicon 2-36, and silicon oxide and/or magnesium perchlorate 2-37. Silicon oxide is taken at ratio 14-37 wt. -% and magnesium perchlorate at ratio 2-5 wt.-%. EFFECT: improved method of silicide producing. Изобретение относится к области неорганической химии, а именно к получению силицида магния, который используется в качестве сырья для получения моноселана. Способ включает приготовление смеси магния, кремния, оксида кремния и/или перхлората магния, термообработку смеси в режиме СВС под давлением инертного газа, преимущественно аргона, равном 0,5 - 2,0 МПа, при следующем соотношении компонентов, мас.%: магний - 60 - 63, кремний - 3,0 - 36, оксид кремния и/или перхлорат магния - 2,0 - 37, при этом оксид кремния берут в количестве 14 - 37 мас.%, а перхлорат магния - 2 - 5 мас.%.