HIGH STRENGTH CORROSION RESISTANT POWDER STEEL

FIELD: iron and steel industry.SUBSTANCE: invention relates to the field of ferrous metallurgy, namely to the production of powder corrosion-resistant martensitic-aging steel used in technologies for the additive production of power elements of gas turbine engines operated at temperatures from -70 t...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Nerush Svyatoslav Vasilevich, Bogachev Igor Aleksandrovich, Tonysheva Olga Aleksandrovna, Krylov Sergej Alekseevich, Kablov Evgenij Nikolaevich, Mazalov Pavel Borisovich
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Nerush Svyatoslav Vasilevich
Bogachev Igor Aleksandrovich
Tonysheva Olga Aleksandrovna
Krylov Sergej Alekseevich
Kablov Evgenij Nikolaevich
Mazalov Pavel Borisovich
description FIELD: iron and steel industry.SUBSTANCE: invention relates to the field of ferrous metallurgy, namely to the production of powder corrosion-resistant martensitic-aging steel used in technologies for the additive production of power elements of gas turbine engines operated at temperatures from -70 to +550°C. Steel contains components in the following ratio, weight percentage: chromium 12.50-13.50, nickel 4.50-5.50, molybdenum 3.50-4.50, cobalt 8.50-9.50, manganese no more than 0.30, silicon no more than 0.10, niobium 0.08-0.15, yttrium no more than 0.02, lanthanum no more than 0.02, carbon no more than 0.02, sulfur no more than 0.01, oxygen no more than 0.06, iron the rest. Steel has a tensile strength of no less than 1400 MPa, a yield strength of no less than 1170 MPa, a relative elongation of no less than 14%, a transverse narrowing of no less than 50%.EFFECT: new high strength steel is obtained.1 cl Изобретение относится к области черной металлургии, а именно к производству порошковой коррозионно-стойкой мартенситно-стареющей стали, используемой в технологиях аддитивного производства силовых элементов газотурбинных двигателей, эксплуатирующихся при температурах от минус 70 до плюс 550°С. Сталь содержит компоненты в следующем соотношении, мас.%: хром 12,50-13,50, никель 4,50-5,50, молибден 3,50-4,50, кобальт 8,50-9,50, марганец не более 0,30, кремний не более 0,10, ниобий 0,08-0,15, иттрий не более 0,02, лантан не более 0,02, углерод не более 0,02, сера не более 0,01, кислород не более 0,06, железо - остальное. Сталь обладает пределом прочности не менее 1400 МПа, пределом текучести не менее 1170 МПа, относительным удлинением не менее 14%, поперечным сужением не менее 50%. 1 з.п. ф-лы, 2 табл.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2751064C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2751064C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2751064C13</originalsourceid><addsrcrecordid>eNrjZNDz8HT3UAgOCXL1cw_xUHD2DwryD_b091MIcg32DA5x9AtRCPAPd3ENAqpxdfXhYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxQaFG5qaGBmYmzobGRCgBAMJKJc8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>HIGH STRENGTH CORROSION RESISTANT POWDER STEEL</title><source>esp@cenet</source><creator>Nerush Svyatoslav Vasilevich ; Bogachev Igor Aleksandrovich ; Tonysheva Olga Aleksandrovna ; Krylov Sergej Alekseevich ; Kablov Evgenij Nikolaevich ; Mazalov Pavel Borisovich</creator><creatorcontrib>Nerush Svyatoslav Vasilevich ; Bogachev Igor Aleksandrovich ; Tonysheva Olga Aleksandrovna ; Krylov Sergej Alekseevich ; Kablov Evgenij Nikolaevich ; Mazalov Pavel Borisovich</creatorcontrib><description>FIELD: iron and steel industry.SUBSTANCE: invention relates to the field of ferrous metallurgy, namely to the production of powder corrosion-resistant martensitic-aging steel used in technologies for the additive production of power elements of gas turbine engines operated at temperatures from -70 to +550°C. Steel contains components in the following ratio, weight percentage: chromium 12.50-13.50, nickel 4.50-5.50, molybdenum 3.50-4.50, cobalt 8.50-9.50, manganese no more than 0.30, silicon no more than 0.10, niobium 0.08-0.15, yttrium no more than 0.02, lanthanum no more than 0.02, carbon no more than 0.02, sulfur no more than 0.01, oxygen no more than 0.06, iron the rest. Steel has a tensile strength of no less than 1400 MPa, a yield strength of no less than 1170 MPa, a relative elongation of no less than 14%, a transverse narrowing of no less than 50%.EFFECT: new high strength steel is obtained.1 cl Изобретение относится к области черной металлургии, а именно к производству порошковой коррозионно-стойкой мартенситно-стареющей стали, используемой в технологиях аддитивного производства силовых элементов газотурбинных двигателей, эксплуатирующихся при температурах от минус 70 до плюс 550°С. Сталь содержит компоненты в следующем соотношении, мас.%: хром 12,50-13,50, никель 4,50-5,50, молибден 3,50-4,50, кобальт 8,50-9,50, марганец не более 0,30, кремний не более 0,10, ниобий 0,08-0,15, иттрий не более 0,02, лантан не более 0,02, углерод не более 0,02, сера не более 0,01, кислород не более 0,06, железо - остальное. Сталь обладает пределом прочности не менее 1400 МПа, пределом текучести не менее 1170 МПа, относительным удлинением не менее 14%, поперечным сужением не менее 50%. 1 з.п. ф-лы, 2 табл.</description><language>eng ; rus</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210707&amp;DB=EPODOC&amp;CC=RU&amp;NR=2751064C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210707&amp;DB=EPODOC&amp;CC=RU&amp;NR=2751064C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Nerush Svyatoslav Vasilevich</creatorcontrib><creatorcontrib>Bogachev Igor Aleksandrovich</creatorcontrib><creatorcontrib>Tonysheva Olga Aleksandrovna</creatorcontrib><creatorcontrib>Krylov Sergej Alekseevich</creatorcontrib><creatorcontrib>Kablov Evgenij Nikolaevich</creatorcontrib><creatorcontrib>Mazalov Pavel Borisovich</creatorcontrib><title>HIGH STRENGTH CORROSION RESISTANT POWDER STEEL</title><description>FIELD: iron and steel industry.SUBSTANCE: invention relates to the field of ferrous metallurgy, namely to the production of powder corrosion-resistant martensitic-aging steel used in technologies for the additive production of power elements of gas turbine engines operated at temperatures from -70 to +550°C. Steel contains components in the following ratio, weight percentage: chromium 12.50-13.50, nickel 4.50-5.50, molybdenum 3.50-4.50, cobalt 8.50-9.50, manganese no more than 0.30, silicon no more than 0.10, niobium 0.08-0.15, yttrium no more than 0.02, lanthanum no more than 0.02, carbon no more than 0.02, sulfur no more than 0.01, oxygen no more than 0.06, iron the rest. Steel has a tensile strength of no less than 1400 MPa, a yield strength of no less than 1170 MPa, a relative elongation of no less than 14%, a transverse narrowing of no less than 50%.EFFECT: new high strength steel is obtained.1 cl Изобретение относится к области черной металлургии, а именно к производству порошковой коррозионно-стойкой мартенситно-стареющей стали, используемой в технологиях аддитивного производства силовых элементов газотурбинных двигателей, эксплуатирующихся при температурах от минус 70 до плюс 550°С. Сталь содержит компоненты в следующем соотношении, мас.%: хром 12,50-13,50, никель 4,50-5,50, молибден 3,50-4,50, кобальт 8,50-9,50, марганец не более 0,30, кремний не более 0,10, ниобий 0,08-0,15, иттрий не более 0,02, лантан не более 0,02, углерод не более 0,02, сера не более 0,01, кислород не более 0,06, железо - остальное. Сталь обладает пределом прочности не менее 1400 МПа, пределом текучести не менее 1170 МПа, относительным удлинением не менее 14%, поперечным сужением не менее 50%. 1 з.п. ф-лы, 2 табл.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNDz8HT3UAgOCXL1cw_xUHD2DwryD_b091MIcg32DA5x9AtRCPAPd3ENAqpxdfXhYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxQaFG5qaGBmYmzobGRCgBAMJKJc8</recordid><startdate>20210707</startdate><enddate>20210707</enddate><creator>Nerush Svyatoslav Vasilevich</creator><creator>Bogachev Igor Aleksandrovich</creator><creator>Tonysheva Olga Aleksandrovna</creator><creator>Krylov Sergej Alekseevich</creator><creator>Kablov Evgenij Nikolaevich</creator><creator>Mazalov Pavel Borisovich</creator><scope>EVB</scope></search><sort><creationdate>20210707</creationdate><title>HIGH STRENGTH CORROSION RESISTANT POWDER STEEL</title><author>Nerush Svyatoslav Vasilevich ; Bogachev Igor Aleksandrovich ; Tonysheva Olga Aleksandrovna ; Krylov Sergej Alekseevich ; Kablov Evgenij Nikolaevich ; Mazalov Pavel Borisovich</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2751064C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2021</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>Nerush Svyatoslav Vasilevich</creatorcontrib><creatorcontrib>Bogachev Igor Aleksandrovich</creatorcontrib><creatorcontrib>Tonysheva Olga Aleksandrovna</creatorcontrib><creatorcontrib>Krylov Sergej Alekseevich</creatorcontrib><creatorcontrib>Kablov Evgenij Nikolaevich</creatorcontrib><creatorcontrib>Mazalov Pavel Borisovich</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Nerush Svyatoslav Vasilevich</au><au>Bogachev Igor Aleksandrovich</au><au>Tonysheva Olga Aleksandrovna</au><au>Krylov Sergej Alekseevich</au><au>Kablov Evgenij Nikolaevich</au><au>Mazalov Pavel Borisovich</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>HIGH STRENGTH CORROSION RESISTANT POWDER STEEL</title><date>2021-07-07</date><risdate>2021</risdate><abstract>FIELD: iron and steel industry.SUBSTANCE: invention relates to the field of ferrous metallurgy, namely to the production of powder corrosion-resistant martensitic-aging steel used in technologies for the additive production of power elements of gas turbine engines operated at temperatures from -70 to +550°C. Steel contains components in the following ratio, weight percentage: chromium 12.50-13.50, nickel 4.50-5.50, molybdenum 3.50-4.50, cobalt 8.50-9.50, manganese no more than 0.30, silicon no more than 0.10, niobium 0.08-0.15, yttrium no more than 0.02, lanthanum no more than 0.02, carbon no more than 0.02, sulfur no more than 0.01, oxygen no more than 0.06, iron the rest. Steel has a tensile strength of no less than 1400 MPa, a yield strength of no less than 1170 MPa, a relative elongation of no less than 14%, a transverse narrowing of no less than 50%.EFFECT: new high strength steel is obtained.1 cl Изобретение относится к области черной металлургии, а именно к производству порошковой коррозионно-стойкой мартенситно-стареющей стали, используемой в технологиях аддитивного производства силовых элементов газотурбинных двигателей, эксплуатирующихся при температурах от минус 70 до плюс 550°С. Сталь содержит компоненты в следующем соотношении, мас.%: хром 12,50-13,50, никель 4,50-5,50, молибден 3,50-4,50, кобальт 8,50-9,50, марганец не более 0,30, кремний не более 0,10, ниобий 0,08-0,15, иттрий не более 0,02, лантан не более 0,02, углерод не более 0,02, сера не более 0,01, кислород не более 0,06, железо - остальное. Сталь обладает пределом прочности не менее 1400 МПа, пределом текучести не менее 1170 МПа, относительным удлинением не менее 14%, поперечным сужением не менее 50%. 1 з.п. ф-лы, 2 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2751064C1
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title HIGH STRENGTH CORROSION RESISTANT POWDER STEEL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-28T16%3A14%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Nerush%20Svyatoslav%20Vasilevich&rft.date=2021-07-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2751064C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true