METHOD FOR THERMAL TREATMENT OF WELDED JOINT ZONE OF DRILLING PIPES

FIELD: metallurgy.SUBSTANCE: to provide strength of welded joint zone of drilling pipes, method involves tempering of welded joint by heating with currents of medium frequency to temperature of 400-450 °C with holding for at least 60 seconds and cooling in calm air, as well as subsequent hardening b...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Kuzmina Elena Aleksandrovna, Atamashkin Artem Sergeevich, Krivov Stepan Aleksandrovich, Priimak Elena Iurevna, Stepanchukova Anna Viktorovna, Medvedev Aleksandr Konstantinovich, Tulibaev Egor Sagitovich
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Kuzmina Elena Aleksandrovna
Atamashkin Artem Sergeevich
Krivov Stepan Aleksandrovich
Priimak Elena Iurevna
Stepanchukova Anna Viktorovna
Medvedev Aleksandr Konstantinovich
Tulibaev Egor Sagitovich
description FIELD: metallurgy.SUBSTANCE: to provide strength of welded joint zone of drilling pipes, method involves tempering of welded joint by heating with currents of medium frequency to temperature of 400-450 °C with holding for at least 60 seconds and cooling in calm air, as well as subsequent hardening by heating high-frequency currents to temperature of Ac+200÷250 °C with cooling in sprayer by water flow.EFFECT: method provides connection of drill pipes without upset parts with locks high resistance to fatigue loads; in addition, reduced power and time costs for production of pipes without upset ends, high technological effectiveness of the process, reduced losses of metal for scaling, maintaining accuracy of pipe geometry.1 cl, 2 tbl Изобретение относится к области металлургии. Для обеспечения прочности зоны сварного соединения бурильных труб способ включает отпуск зоны сварного соединения путем нагрева токами средней частоты до температуры 400-450°C с выдержкой не менее 60 секунд и охлаждением на спокойном воздухе, а также последующую закалку нагревом токами высокой частоты до температуры Ас+200÷250°C с охлаждением в спрейере потоком воды. Способ обеспечивает соединениям бурильных труб без высаженных частей с замками высокое сопротивление усталостным нагрузкам. Кроме того, выявлено снижение энергетических и временных затрат на производство труб без высаженных концов, повышение технологичности процесса, снижение потерь металла на окалинообразование, сохранение точности геометрии труб. 2 табл.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2726209C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2726209C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2726209C13</originalsourceid><addsrcrecordid>eNrjZHD2dQ3x8HdRcPMPUgjxcA3ydfRRCAlydQzxdfULUfB3Uwh39XFxdVHw8vcE8qP8_VxBgi5Bnj4-nn7uCgGeAa7BPAysaYk5xam8UJqbQcHNNcTZQze1ID8-tbggMTk1L7UkPijUyNzIzMjA0tnQmAglAMefKxA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR THERMAL TREATMENT OF WELDED JOINT ZONE OF DRILLING PIPES</title><source>esp@cenet</source><creator>Kuzmina Elena Aleksandrovna ; Atamashkin Artem Sergeevich ; Krivov Stepan Aleksandrovich ; Priimak Elena Iurevna ; Stepanchukova Anna Viktorovna ; Medvedev Aleksandr Konstantinovich ; Tulibaev Egor Sagitovich</creator><creatorcontrib>Kuzmina Elena Aleksandrovna ; Atamashkin Artem Sergeevich ; Krivov Stepan Aleksandrovich ; Priimak Elena Iurevna ; Stepanchukova Anna Viktorovna ; Medvedev Aleksandr Konstantinovich ; Tulibaev Egor Sagitovich</creatorcontrib><description>FIELD: metallurgy.SUBSTANCE: to provide strength of welded joint zone of drilling pipes, method involves tempering of welded joint by heating with currents of medium frequency to temperature of 400-450 °C with holding for at least 60 seconds and cooling in calm air, as well as subsequent hardening by heating high-frequency currents to temperature of Ac+200÷250 °C with cooling in sprayer by water flow.EFFECT: method provides connection of drill pipes without upset parts with locks high resistance to fatigue loads; in addition, reduced power and time costs for production of pipes without upset ends, high technological effectiveness of the process, reduced losses of metal for scaling, maintaining accuracy of pipe geometry.1 cl, 2 tbl Изобретение относится к области металлургии. Для обеспечения прочности зоны сварного соединения бурильных труб способ включает отпуск зоны сварного соединения путем нагрева токами средней частоты до температуры 400-450°C с выдержкой не менее 60 секунд и охлаждением на спокойном воздухе, а также последующую закалку нагревом токами высокой частоты до температуры Ас+200÷250°C с охлаждением в спрейере потоком воды. Способ обеспечивает соединениям бурильных труб без высаженных частей с замками высокое сопротивление усталостным нагрузкам. Кроме того, выявлено снижение энергетических и временных затрат на производство труб без высаженных концов, повышение технологичности процесса, снижение потерь металла на окалинообразование, сохранение точности геометрии труб. 2 табл.</description><language>eng ; rus</language><subject>CHEMISTRY ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200709&amp;DB=EPODOC&amp;CC=RU&amp;NR=2726209C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200709&amp;DB=EPODOC&amp;CC=RU&amp;NR=2726209C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Kuzmina Elena Aleksandrovna</creatorcontrib><creatorcontrib>Atamashkin Artem Sergeevich</creatorcontrib><creatorcontrib>Krivov Stepan Aleksandrovich</creatorcontrib><creatorcontrib>Priimak Elena Iurevna</creatorcontrib><creatorcontrib>Stepanchukova Anna Viktorovna</creatorcontrib><creatorcontrib>Medvedev Aleksandr Konstantinovich</creatorcontrib><creatorcontrib>Tulibaev Egor Sagitovich</creatorcontrib><title>METHOD FOR THERMAL TREATMENT OF WELDED JOINT ZONE OF DRILLING PIPES</title><description>FIELD: metallurgy.SUBSTANCE: to provide strength of welded joint zone of drilling pipes, method involves tempering of welded joint by heating with currents of medium frequency to temperature of 400-450 °C with holding for at least 60 seconds and cooling in calm air, as well as subsequent hardening by heating high-frequency currents to temperature of Ac+200÷250 °C with cooling in sprayer by water flow.EFFECT: method provides connection of drill pipes without upset parts with locks high resistance to fatigue loads; in addition, reduced power and time costs for production of pipes without upset ends, high technological effectiveness of the process, reduced losses of metal for scaling, maintaining accuracy of pipe geometry.1 cl, 2 tbl Изобретение относится к области металлургии. Для обеспечения прочности зоны сварного соединения бурильных труб способ включает отпуск зоны сварного соединения путем нагрева токами средней частоты до температуры 400-450°C с выдержкой не менее 60 секунд и охлаждением на спокойном воздухе, а также последующую закалку нагревом токами высокой частоты до температуры Ас+200÷250°C с охлаждением в спрейере потоком воды. Способ обеспечивает соединениям бурильных труб без высаженных частей с замками высокое сопротивление усталостным нагрузкам. Кроме того, выявлено снижение энергетических и временных затрат на производство труб без высаженных концов, повышение технологичности процесса, снижение потерь металла на окалинообразование, сохранение точности геометрии труб. 2 табл.</description><subject>CHEMISTRY</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD2dQ3x8HdRcPMPUgjxcA3ydfRRCAlydQzxdfULUfB3Uwh39XFxdVHw8vcE8qP8_VxBgi5Bnj4-nn7uCgGeAa7BPAysaYk5xam8UJqbQcHNNcTZQze1ID8-tbggMTk1L7UkPijUyNzIzMjA0tnQmAglAMefKxA</recordid><startdate>20200709</startdate><enddate>20200709</enddate><creator>Kuzmina Elena Aleksandrovna</creator><creator>Atamashkin Artem Sergeevich</creator><creator>Krivov Stepan Aleksandrovich</creator><creator>Priimak Elena Iurevna</creator><creator>Stepanchukova Anna Viktorovna</creator><creator>Medvedev Aleksandr Konstantinovich</creator><creator>Tulibaev Egor Sagitovich</creator><scope>EVB</scope></search><sort><creationdate>20200709</creationdate><title>METHOD FOR THERMAL TREATMENT OF WELDED JOINT ZONE OF DRILLING PIPES</title><author>Kuzmina Elena Aleksandrovna ; Atamashkin Artem Sergeevich ; Krivov Stepan Aleksandrovich ; Priimak Elena Iurevna ; Stepanchukova Anna Viktorovna ; Medvedev Aleksandr Konstantinovich ; Tulibaev Egor Sagitovich</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2726209C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2020</creationdate><topic>CHEMISTRY</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>Kuzmina Elena Aleksandrovna</creatorcontrib><creatorcontrib>Atamashkin Artem Sergeevich</creatorcontrib><creatorcontrib>Krivov Stepan Aleksandrovich</creatorcontrib><creatorcontrib>Priimak Elena Iurevna</creatorcontrib><creatorcontrib>Stepanchukova Anna Viktorovna</creatorcontrib><creatorcontrib>Medvedev Aleksandr Konstantinovich</creatorcontrib><creatorcontrib>Tulibaev Egor Sagitovich</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Kuzmina Elena Aleksandrovna</au><au>Atamashkin Artem Sergeevich</au><au>Krivov Stepan Aleksandrovich</au><au>Priimak Elena Iurevna</au><au>Stepanchukova Anna Viktorovna</au><au>Medvedev Aleksandr Konstantinovich</au><au>Tulibaev Egor Sagitovich</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR THERMAL TREATMENT OF WELDED JOINT ZONE OF DRILLING PIPES</title><date>2020-07-09</date><risdate>2020</risdate><abstract>FIELD: metallurgy.SUBSTANCE: to provide strength of welded joint zone of drilling pipes, method involves tempering of welded joint by heating with currents of medium frequency to temperature of 400-450 °C with holding for at least 60 seconds and cooling in calm air, as well as subsequent hardening by heating high-frequency currents to temperature of Ac+200÷250 °C with cooling in sprayer by water flow.EFFECT: method provides connection of drill pipes without upset parts with locks high resistance to fatigue loads; in addition, reduced power and time costs for production of pipes without upset ends, high technological effectiveness of the process, reduced losses of metal for scaling, maintaining accuracy of pipe geometry.1 cl, 2 tbl Изобретение относится к области металлургии. Для обеспечения прочности зоны сварного соединения бурильных труб способ включает отпуск зоны сварного соединения путем нагрева токами средней частоты до температуры 400-450°C с выдержкой не менее 60 секунд и охлаждением на спокойном воздухе, а также последующую закалку нагревом токами высокой частоты до температуры Ас+200÷250°C с охлаждением в спрейере потоком воды. Способ обеспечивает соединениям бурильных труб без высаженных частей с замками высокое сопротивление усталостным нагрузкам. Кроме того, выявлено снижение энергетических и временных затрат на производство труб без высаженных концов, повышение технологичности процесса, снижение потерь металла на окалинообразование, сохранение точности геометрии труб. 2 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2726209C1
source esp@cenet
subjects CHEMISTRY
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
title METHOD FOR THERMAL TREATMENT OF WELDED JOINT ZONE OF DRILLING PIPES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T00%3A21%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Kuzmina%20Elena%20Aleksandrovna&rft.date=2020-07-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2726209C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true