METHOD OF WOOD IMPREGNATION
FIELD: woodworking industry.SUBSTANCE: invention relates to woodworking industry, in particular, to impregnation of wood with pre-drying. Wood is heated to bulk volume temperature 80-100 °C and immersed in impregnation liquid. Prior to immersion, partial drying of wood is performed with loss of 5-20...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: woodworking industry.SUBSTANCE: invention relates to woodworking industry, in particular, to impregnation of wood with pre-drying. Wood is heated to bulk volume temperature 80-100 °C and immersed in impregnation liquid. Prior to immersion, partial drying of wood is performed with loss of 5-20 % of moisture contained in wood before drying. At that time interval after completion of incomplete drying and immersion into impregnating liquid ranges from 1 to 60 s, and duration of impregnation makes 10 to 60 minutes.EFFECT: simplified process of wood impregnation.1 cl, 1 dwg
Изобретение относится к деревообрабатывающей промышленности, в частности к пропитке древесины с предварительной сушкой. Выполняют нагрев древесины до среднеобъемной температуры 80-100°C и погружение в пропиточную жидкость. Перед погружением выполняют неполную сушку древесины с потерей от 5 до 20% влаги, содержавшейся в древесине перед сушкой. При этом интервал времени после завершения неполной сушки и погружением в пропиточную жидкость составляет от 1 до 60 с, а продолжительность пропитывания составляет от 10 до 60 мин. Упрощается процесс пропитки древесины. 1 ил. |
---|