METHOD OF OBTAINING COATINGS FOR ITEMS MADE OF VALVE METAL ALLOYS

FIELD: technological processes.SUBSTANCE: invention relates to the field of electroplating and can be used in mechanical engineering and related industries. Method includes electrochemical oxidation with a duration of 30-100 minutes in reverse flows of acidic or alkaline electrolyte solutions, where...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Tsibizov Pavel Nikolaevich, Chufistov Oleg Evgenevich, Zharkov Mikhail Sergeevich, Filatov Pavel Mikhajlovich, Chufistov Evgenij Alekseevich
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Tsibizov Pavel Nikolaevich
Chufistov Oleg Evgenevich
Zharkov Mikhail Sergeevich
Filatov Pavel Mikhajlovich
Chufistov Evgenij Alekseevich
description FIELD: technological processes.SUBSTANCE: invention relates to the field of electroplating and can be used in mechanical engineering and related industries. Method includes electrochemical oxidation with a duration of 30-100 minutes in reverse flows of acidic or alkaline electrolyte solutions, wherein oxidation is carried out without the use of special baths, installing parts inside the counter-electrodes of stainless steel, in cavities, the shapes of which correspond to the shapes of the parts, and the dimensions exceed the corresponding external dimensions of parts by 4-10 mm, while electrolyte solutions are passed through these cavities, ensuring their consumption from 0.2 to 5.0 liters per 1 dmthe area of the oxidized surfaces of the parts and changing the direction of their flow on the opposite, after half the time of oxidation.EFFECT: obtaining high-quality uniform coatings on surfaces of parts with low-tech surface areas.1 cl, 2 dwg, 2 tbl Изобретение относится к области гальванотехники и может быть использовано в машиностроении и смежных отраслях промышленности. Способ включает электрохимическое оксидирование продолжительностью 30-100 минут в реверсивных потоках кислых или щелочных растворов электролитов, при этом оксидирование осуществляют без применения специальных ванн, устанавливая детали внутри противоэлектродов из нержавеющей стали, в полостях, формы которых соответствуют формам деталей, а размеры превышают соответствующие наружные размеры деталей на 4-10 мм, при этом через данные полости пропускают растворы электролитов, обеспечивая их расход от 0,2 до 5,0 л на 1 дмплощади оксидируемых поверхностей деталей и изменяя направление их течения на противоположное, спустя половину времени оксидирования. Технический результат: получение качественных равномерных покрытий на поверхностях деталей с нетехнологичными участками поверхностей. 2 ил., 2 табл.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2676380C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2676380C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2676380C13</originalsourceid><addsrcrecordid>eNrjZHD0dQ3x8HdR8HdT8HcKcfT08_RzV3D2dwwB0sEKbv5BCp4hrr7BCr6OLq4gRWGOPmGuCkBNjj4Kjj4-_pHBPAysaYk5xam8UJqbQcHNNcTZQze1ID8-tbggMTk1L7UkPijUyMzczNjCwNnQmAglAFw8Kls</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF OBTAINING COATINGS FOR ITEMS MADE OF VALVE METAL ALLOYS</title><source>esp@cenet</source><creator>Tsibizov Pavel Nikolaevich ; Chufistov Oleg Evgenevich ; Zharkov Mikhail Sergeevich ; Filatov Pavel Mikhajlovich ; Chufistov Evgenij Alekseevich</creator><creatorcontrib>Tsibizov Pavel Nikolaevich ; Chufistov Oleg Evgenevich ; Zharkov Mikhail Sergeevich ; Filatov Pavel Mikhajlovich ; Chufistov Evgenij Alekseevich</creatorcontrib><description>FIELD: technological processes.SUBSTANCE: invention relates to the field of electroplating and can be used in mechanical engineering and related industries. Method includes electrochemical oxidation with a duration of 30-100 minutes in reverse flows of acidic or alkaline electrolyte solutions, wherein oxidation is carried out without the use of special baths, installing parts inside the counter-electrodes of stainless steel, in cavities, the shapes of which correspond to the shapes of the parts, and the dimensions exceed the corresponding external dimensions of parts by 4-10 mm, while electrolyte solutions are passed through these cavities, ensuring their consumption from 0.2 to 5.0 liters per 1 dmthe area of the oxidized surfaces of the parts and changing the direction of their flow on the opposite, after half the time of oxidation.EFFECT: obtaining high-quality uniform coatings on surfaces of parts with low-tech surface areas.1 cl, 2 dwg, 2 tbl Изобретение относится к области гальванотехники и может быть использовано в машиностроении и смежных отраслях промышленности. Способ включает электрохимическое оксидирование продолжительностью 30-100 минут в реверсивных потоках кислых или щелочных растворов электролитов, при этом оксидирование осуществляют без применения специальных ванн, устанавливая детали внутри противоэлектродов из нержавеющей стали, в полостях, формы которых соответствуют формам деталей, а размеры превышают соответствующие наружные размеры деталей на 4-10 мм, при этом через данные полости пропускают растворы электролитов, обеспечивая их расход от 0,2 до 5,0 л на 1 дмплощади оксидируемых поверхностей деталей и изменяя направление их течения на противоположное, спустя половину времени оксидирования. Технический результат: получение качественных равномерных покрытий на поверхностях деталей с нетехнологичными участками поверхностей. 2 ил., 2 табл.</description><language>eng ; rus</language><subject>APPARATUS THEREFOR ; CHEMISTRY ; ELECTROFORMING ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; METALLURGY ; PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20181228&amp;DB=EPODOC&amp;CC=RU&amp;NR=2676380C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20181228&amp;DB=EPODOC&amp;CC=RU&amp;NR=2676380C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Tsibizov Pavel Nikolaevich</creatorcontrib><creatorcontrib>Chufistov Oleg Evgenevich</creatorcontrib><creatorcontrib>Zharkov Mikhail Sergeevich</creatorcontrib><creatorcontrib>Filatov Pavel Mikhajlovich</creatorcontrib><creatorcontrib>Chufistov Evgenij Alekseevich</creatorcontrib><title>METHOD OF OBTAINING COATINGS FOR ITEMS MADE OF VALVE METAL ALLOYS</title><description>FIELD: technological processes.SUBSTANCE: invention relates to the field of electroplating and can be used in mechanical engineering and related industries. Method includes electrochemical oxidation with a duration of 30-100 minutes in reverse flows of acidic or alkaline electrolyte solutions, wherein oxidation is carried out without the use of special baths, installing parts inside the counter-electrodes of stainless steel, in cavities, the shapes of which correspond to the shapes of the parts, and the dimensions exceed the corresponding external dimensions of parts by 4-10 mm, while electrolyte solutions are passed through these cavities, ensuring their consumption from 0.2 to 5.0 liters per 1 dmthe area of the oxidized surfaces of the parts and changing the direction of their flow on the opposite, after half the time of oxidation.EFFECT: obtaining high-quality uniform coatings on surfaces of parts with low-tech surface areas.1 cl, 2 dwg, 2 tbl Изобретение относится к области гальванотехники и может быть использовано в машиностроении и смежных отраслях промышленности. Способ включает электрохимическое оксидирование продолжительностью 30-100 минут в реверсивных потоках кислых или щелочных растворов электролитов, при этом оксидирование осуществляют без применения специальных ванн, устанавливая детали внутри противоэлектродов из нержавеющей стали, в полостях, формы которых соответствуют формам деталей, а размеры превышают соответствующие наружные размеры деталей на 4-10 мм, при этом через данные полости пропускают растворы электролитов, обеспечивая их расход от 0,2 до 5,0 л на 1 дмплощади оксидируемых поверхностей деталей и изменяя направление их течения на противоположное, спустя половину времени оксидирования. Технический результат: получение качественных равномерных покрытий на поверхностях деталей с нетехнологичными участками поверхностей. 2 ил., 2 табл.</description><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>ELECTROFORMING</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>METALLURGY</subject><subject>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD0dQ3x8HdR8HdT8HcKcfT08_RzV3D2dwwB0sEKbv5BCp4hrr7BCr6OLq4gRWGOPmGuCkBNjj4Kjj4-_pHBPAysaYk5xam8UJqbQcHNNcTZQze1ID8-tbggMTk1L7UkPijUyMzczNjCwNnQmAglAFw8Kls</recordid><startdate>20181228</startdate><enddate>20181228</enddate><creator>Tsibizov Pavel Nikolaevich</creator><creator>Chufistov Oleg Evgenevich</creator><creator>Zharkov Mikhail Sergeevich</creator><creator>Filatov Pavel Mikhajlovich</creator><creator>Chufistov Evgenij Alekseevich</creator><scope>EVB</scope></search><sort><creationdate>20181228</creationdate><title>METHOD OF OBTAINING COATINGS FOR ITEMS MADE OF VALVE METAL ALLOYS</title><author>Tsibizov Pavel Nikolaevich ; Chufistov Oleg Evgenevich ; Zharkov Mikhail Sergeevich ; Filatov Pavel Mikhajlovich ; Chufistov Evgenij Alekseevich</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2676380C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2018</creationdate><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>ELECTROFORMING</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>METALLURGY</topic><topic>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</topic><toplevel>online_resources</toplevel><creatorcontrib>Tsibizov Pavel Nikolaevich</creatorcontrib><creatorcontrib>Chufistov Oleg Evgenevich</creatorcontrib><creatorcontrib>Zharkov Mikhail Sergeevich</creatorcontrib><creatorcontrib>Filatov Pavel Mikhajlovich</creatorcontrib><creatorcontrib>Chufistov Evgenij Alekseevich</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Tsibizov Pavel Nikolaevich</au><au>Chufistov Oleg Evgenevich</au><au>Zharkov Mikhail Sergeevich</au><au>Filatov Pavel Mikhajlovich</au><au>Chufistov Evgenij Alekseevich</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF OBTAINING COATINGS FOR ITEMS MADE OF VALVE METAL ALLOYS</title><date>2018-12-28</date><risdate>2018</risdate><abstract>FIELD: technological processes.SUBSTANCE: invention relates to the field of electroplating and can be used in mechanical engineering and related industries. Method includes electrochemical oxidation with a duration of 30-100 minutes in reverse flows of acidic or alkaline electrolyte solutions, wherein oxidation is carried out without the use of special baths, installing parts inside the counter-electrodes of stainless steel, in cavities, the shapes of which correspond to the shapes of the parts, and the dimensions exceed the corresponding external dimensions of parts by 4-10 mm, while electrolyte solutions are passed through these cavities, ensuring their consumption from 0.2 to 5.0 liters per 1 dmthe area of the oxidized surfaces of the parts and changing the direction of their flow on the opposite, after half the time of oxidation.EFFECT: obtaining high-quality uniform coatings on surfaces of parts with low-tech surface areas.1 cl, 2 dwg, 2 tbl Изобретение относится к области гальванотехники и может быть использовано в машиностроении и смежных отраслях промышленности. Способ включает электрохимическое оксидирование продолжительностью 30-100 минут в реверсивных потоках кислых или щелочных растворов электролитов, при этом оксидирование осуществляют без применения специальных ванн, устанавливая детали внутри противоэлектродов из нержавеющей стали, в полостях, формы которых соответствуют формам деталей, а размеры превышают соответствующие наружные размеры деталей на 4-10 мм, при этом через данные полости пропускают растворы электролитов, обеспечивая их расход от 0,2 до 5,0 л на 1 дмплощади оксидируемых поверхностей деталей и изменяя направление их течения на противоположное, спустя половину времени оксидирования. Технический результат: получение качественных равномерных покрытий на поверхностях деталей с нетехнологичными участками поверхностей. 2 ил., 2 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2676380C1
source esp@cenet
subjects APPARATUS THEREFOR
CHEMISTRY
ELECTROFORMING
ELECTROLYTIC OR ELECTROPHORETIC PROCESSES
METALLURGY
PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS
title METHOD OF OBTAINING COATINGS FOR ITEMS MADE OF VALVE METAL ALLOYS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-24T13%3A30%3A42IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Tsibizov%20Pavel%20Nikolaevich&rft.date=2018-12-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2676380C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true