METHOD OF IMPREGNATION FROM POROUS CARBON-CARBON COMPOSITE MATERIAL
FIELD: chemistry.SUBSTANCE: invention relates to structural materials operating in conditions of high thermal load and oxidative medium, and can be used in chemical, petrochemical and chemical-metallurgical industry, as well as aircraft engineering. In the method for impregnating articles from a por...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | Anikin Vyacheslav Nikolaevich Chuprunov Konstantin Olegovich Zolotareva Kristina Anatolevna Fanaskova Natalya Vyacheslavovna Guskov Vladimir Nikolaevich Anikin Grigorij Vyacheslavovich Eremin Sergej Aleksandrovich Kuznetsov Denis Valerevich Kryuchkov Konstantin Viktorovich Tambovtseva Alla Agonesovna |
description | FIELD: chemistry.SUBSTANCE: invention relates to structural materials operating in conditions of high thermal load and oxidative medium, and can be used in chemical, petrochemical and chemical-metallurgical industry, as well as aircraft engineering. In the method for impregnating articles from a porous carbon-carbon composite material comprising treating carbon-fiber products with tantalum chloride in the presence of methane on heating, the impregnation is carried out by chemical vapor deposition in an inert medium at a product heating temperature of up to 940-970°C, and tantalum chloride - up to 180-210°C. The concentration of tantalum chloride is 0.2-0.5 g/l, and the methane consumption is 0.07-0.18 l/min.EFFECT: obtaining a product with high oxidation resistance by forming a protective barrier layer on its surface, which allows uniform redistribution of internal thermal stresses arising during heating.1 ex, 1 tbl
Предлагаемое изобретение относится к области конструкционных материалов, работающих в условиях высокого теплового нагружения и окислительной среды и может быть использовано в химической, нефтехимической и химико-металлургической отраслях промышленности. В способе пропитки изделий из пористого углерод-углеродного композиционного материала, включающем обработку изделий на основе углеродного волокна хлоридом тантала в присутствии метана при нагревании, пропитку проводят методом химического осаждения из газовой фазы в инертной среде при температуре нагрева изделия до 940-970°С, а хлорида тантала - до 180-210°С. Концентрация хлорида тантала составляет 0,2-0,5 г/л, а расход метана 0,07-0,18 л/мин. Технический результат изобретения - получение изделия с высокой окислительной стойкостью за счет образования защитного барьерного слоя на его поверхности, позволяющего равномерно перераспределять внутренние термические напряжения, возникающие при нагреве. 1 пр., 1 табл. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2622061C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2622061C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2622061C13</originalsourceid><addsrcrecordid>eNrjZHD2dQ3x8HdR8HdT8PQNCHJ193MM8fT3U3AL8vdVCPAP8g8NVnB2DHLy99OFUArO_r4B_sGeIa4Kvo4hrkGejj48DKxpiTnFqbxQmptBwc01xNlDN7UgPz61uCAxOTUvtSQ-KNTIzMjIwMzQ2dCYCCUA7SYrWA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF IMPREGNATION FROM POROUS CARBON-CARBON COMPOSITE MATERIAL</title><source>esp@cenet</source><creator>Anikin Vyacheslav Nikolaevich ; Chuprunov Konstantin Olegovich ; Zolotareva Kristina Anatolevna ; Fanaskova Natalya Vyacheslavovna ; Guskov Vladimir Nikolaevich ; Anikin Grigorij Vyacheslavovich ; Eremin Sergej Aleksandrovich ; Kuznetsov Denis Valerevich ; Kryuchkov Konstantin Viktorovich ; Tambovtseva Alla Agonesovna</creator><creatorcontrib>Anikin Vyacheslav Nikolaevich ; Chuprunov Konstantin Olegovich ; Zolotareva Kristina Anatolevna ; Fanaskova Natalya Vyacheslavovna ; Guskov Vladimir Nikolaevich ; Anikin Grigorij Vyacheslavovich ; Eremin Sergej Aleksandrovich ; Kuznetsov Denis Valerevich ; Kryuchkov Konstantin Viktorovich ; Tambovtseva Alla Agonesovna</creatorcontrib><description>FIELD: chemistry.SUBSTANCE: invention relates to structural materials operating in conditions of high thermal load and oxidative medium, and can be used in chemical, petrochemical and chemical-metallurgical industry, as well as aircraft engineering. In the method for impregnating articles from a porous carbon-carbon composite material comprising treating carbon-fiber products with tantalum chloride in the presence of methane on heating, the impregnation is carried out by chemical vapor deposition in an inert medium at a product heating temperature of up to 940-970°C, and tantalum chloride - up to 180-210°C. The concentration of tantalum chloride is 0.2-0.5 g/l, and the methane consumption is 0.07-0.18 l/min.EFFECT: obtaining a product with high oxidation resistance by forming a protective barrier layer on its surface, which allows uniform redistribution of internal thermal stresses arising during heating.1 ex, 1 tbl
Предлагаемое изобретение относится к области конструкционных материалов, работающих в условиях высокого теплового нагружения и окислительной среды и может быть использовано в химической, нефтехимической и химико-металлургической отраслях промышленности. В способе пропитки изделий из пористого углерод-углеродного композиционного материала, включающем обработку изделий на основе углеродного волокна хлоридом тантала в присутствии метана при нагревании, пропитку проводят методом химического осаждения из газовой фазы в инертной среде при температуре нагрева изделия до 940-970°С, а хлорида тантала - до 180-210°С. Концентрация хлорида тантала составляет 0,2-0,5 г/л, а расход метана 0,07-0,18 л/мин. Технический результат изобретения - получение изделия с высокой окислительной стойкостью за счет образования защитного барьерного слоя на его поверхности, позволяющего равномерно перераспределять внутренние термические напряжения, возникающие при нагреве. 1 пр., 1 табл.</description><language>eng ; rus</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20170609&DB=EPODOC&CC=RU&NR=2622061C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20170609&DB=EPODOC&CC=RU&NR=2622061C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Anikin Vyacheslav Nikolaevich</creatorcontrib><creatorcontrib>Chuprunov Konstantin Olegovich</creatorcontrib><creatorcontrib>Zolotareva Kristina Anatolevna</creatorcontrib><creatorcontrib>Fanaskova Natalya Vyacheslavovna</creatorcontrib><creatorcontrib>Guskov Vladimir Nikolaevich</creatorcontrib><creatorcontrib>Anikin Grigorij Vyacheslavovich</creatorcontrib><creatorcontrib>Eremin Sergej Aleksandrovich</creatorcontrib><creatorcontrib>Kuznetsov Denis Valerevich</creatorcontrib><creatorcontrib>Kryuchkov Konstantin Viktorovich</creatorcontrib><creatorcontrib>Tambovtseva Alla Agonesovna</creatorcontrib><title>METHOD OF IMPREGNATION FROM POROUS CARBON-CARBON COMPOSITE MATERIAL</title><description>FIELD: chemistry.SUBSTANCE: invention relates to structural materials operating in conditions of high thermal load and oxidative medium, and can be used in chemical, petrochemical and chemical-metallurgical industry, as well as aircraft engineering. In the method for impregnating articles from a porous carbon-carbon composite material comprising treating carbon-fiber products with tantalum chloride in the presence of methane on heating, the impregnation is carried out by chemical vapor deposition in an inert medium at a product heating temperature of up to 940-970°C, and tantalum chloride - up to 180-210°C. The concentration of tantalum chloride is 0.2-0.5 g/l, and the methane consumption is 0.07-0.18 l/min.EFFECT: obtaining a product with high oxidation resistance by forming a protective barrier layer on its surface, which allows uniform redistribution of internal thermal stresses arising during heating.1 ex, 1 tbl
Предлагаемое изобретение относится к области конструкционных материалов, работающих в условиях высокого теплового нагружения и окислительной среды и может быть использовано в химической, нефтехимической и химико-металлургической отраслях промышленности. В способе пропитки изделий из пористого углерод-углеродного композиционного материала, включающем обработку изделий на основе углеродного волокна хлоридом тантала в присутствии метана при нагревании, пропитку проводят методом химического осаждения из газовой фазы в инертной среде при температуре нагрева изделия до 940-970°С, а хлорида тантала - до 180-210°С. Концентрация хлорида тантала составляет 0,2-0,5 г/л, а расход метана 0,07-0,18 л/мин. Технический результат изобретения - получение изделия с высокой окислительной стойкостью за счет образования защитного барьерного слоя на его поверхности, позволяющего равномерно перераспределять внутренние термические напряжения, возникающие при нагреве. 1 пр., 1 табл.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD2dQ3x8HdR8HdT8PQNCHJ193MM8fT3U3AL8vdVCPAP8g8NVnB2DHLy99OFUArO_r4B_sGeIa4Kvo4hrkGejj48DKxpiTnFqbxQmptBwc01xNlDN7UgPz61uCAxOTUvtSQ-KNTIzMjIwMzQ2dCYCCUA7SYrWA</recordid><startdate>20170609</startdate><enddate>20170609</enddate><creator>Anikin Vyacheslav Nikolaevich</creator><creator>Chuprunov Konstantin Olegovich</creator><creator>Zolotareva Kristina Anatolevna</creator><creator>Fanaskova Natalya Vyacheslavovna</creator><creator>Guskov Vladimir Nikolaevich</creator><creator>Anikin Grigorij Vyacheslavovich</creator><creator>Eremin Sergej Aleksandrovich</creator><creator>Kuznetsov Denis Valerevich</creator><creator>Kryuchkov Konstantin Viktorovich</creator><creator>Tambovtseva Alla Agonesovna</creator><scope>EVB</scope></search><sort><creationdate>20170609</creationdate><title>METHOD OF IMPREGNATION FROM POROUS CARBON-CARBON COMPOSITE MATERIAL</title><author>Anikin Vyacheslav Nikolaevich ; Chuprunov Konstantin Olegovich ; Zolotareva Kristina Anatolevna ; Fanaskova Natalya Vyacheslavovna ; Guskov Vladimir Nikolaevich ; Anikin Grigorij Vyacheslavovich ; Eremin Sergej Aleksandrovich ; Kuznetsov Denis Valerevich ; Kryuchkov Konstantin Viktorovich ; Tambovtseva Alla Agonesovna</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2622061C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2017</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>Anikin Vyacheslav Nikolaevich</creatorcontrib><creatorcontrib>Chuprunov Konstantin Olegovich</creatorcontrib><creatorcontrib>Zolotareva Kristina Anatolevna</creatorcontrib><creatorcontrib>Fanaskova Natalya Vyacheslavovna</creatorcontrib><creatorcontrib>Guskov Vladimir Nikolaevich</creatorcontrib><creatorcontrib>Anikin Grigorij Vyacheslavovich</creatorcontrib><creatorcontrib>Eremin Sergej Aleksandrovich</creatorcontrib><creatorcontrib>Kuznetsov Denis Valerevich</creatorcontrib><creatorcontrib>Kryuchkov Konstantin Viktorovich</creatorcontrib><creatorcontrib>Tambovtseva Alla Agonesovna</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Anikin Vyacheslav Nikolaevich</au><au>Chuprunov Konstantin Olegovich</au><au>Zolotareva Kristina Anatolevna</au><au>Fanaskova Natalya Vyacheslavovna</au><au>Guskov Vladimir Nikolaevich</au><au>Anikin Grigorij Vyacheslavovich</au><au>Eremin Sergej Aleksandrovich</au><au>Kuznetsov Denis Valerevich</au><au>Kryuchkov Konstantin Viktorovich</au><au>Tambovtseva Alla Agonesovna</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF IMPREGNATION FROM POROUS CARBON-CARBON COMPOSITE MATERIAL</title><date>2017-06-09</date><risdate>2017</risdate><abstract>FIELD: chemistry.SUBSTANCE: invention relates to structural materials operating in conditions of high thermal load and oxidative medium, and can be used in chemical, petrochemical and chemical-metallurgical industry, as well as aircraft engineering. In the method for impregnating articles from a porous carbon-carbon composite material comprising treating carbon-fiber products with tantalum chloride in the presence of methane on heating, the impregnation is carried out by chemical vapor deposition in an inert medium at a product heating temperature of up to 940-970°C, and tantalum chloride - up to 180-210°C. The concentration of tantalum chloride is 0.2-0.5 g/l, and the methane consumption is 0.07-0.18 l/min.EFFECT: obtaining a product with high oxidation resistance by forming a protective barrier layer on its surface, which allows uniform redistribution of internal thermal stresses arising during heating.1 ex, 1 tbl
Предлагаемое изобретение относится к области конструкционных материалов, работающих в условиях высокого теплового нагружения и окислительной среды и может быть использовано в химической, нефтехимической и химико-металлургической отраслях промышленности. В способе пропитки изделий из пористого углерод-углеродного композиционного материала, включающем обработку изделий на основе углеродного волокна хлоридом тантала в присутствии метана при нагревании, пропитку проводят методом химического осаждения из газовой фазы в инертной среде при температуре нагрева изделия до 940-970°С, а хлорида тантала - до 180-210°С. Концентрация хлорида тантала составляет 0,2-0,5 г/л, а расход метана 0,07-0,18 л/мин. Технический результат изобретения - получение изделия с высокой окислительной стойкостью за счет образования защитного барьерного слоя на его поверхности, позволяющего равномерно перераспределять внутренние термические напряжения, возникающие при нагреве. 1 пр., 1 табл.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; rus |
recordid | cdi_epo_espacenet_RU2622061C1 |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE LIME, MAGNESIA METALLURGY REFRACTORIES SLAG TREATMENT OF NATURAL STONE |
title | METHOD OF IMPREGNATION FROM POROUS CARBON-CARBON COMPOSITE MATERIAL |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T22%3A55%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Anikin%20Vyacheslav%20Nikolaevich&rft.date=2017-06-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2622061C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |