METHOD OF PREPARING BASE POLYMER SOLUTION FOR PRODUCING HALOBUTYL RUBBER

FIELD: chemistry.SUBSTANCE: method is done by dissolving the moist crumb butyl rubber in hydrocarbon solvents by filing a moist crumb rubber, solvent, the filing and withdrawal solution base polymer and water output in the hollow device. While the device has a zone of mixing, dissolving and settling...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Khabibullin Rafik Khatmullaevich, Mironov Igor Vasilevich, Aglyamov Irek Angamovich, Sofronova Olga Vladimirovna, Gazetdinov Ajdar Khanifovich, Kubanov Kirill Mikhajlovich, Poretskov Anatolij Yurevich, Nesterov Oleg Nikolaevich, Gavrikov Viktor Nikolaevich, Sakhabutdinov Anas Gaptynurovich
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Khabibullin Rafik Khatmullaevich
Mironov Igor Vasilevich
Aglyamov Irek Angamovich
Sofronova Olga Vladimirovna
Gazetdinov Ajdar Khanifovich
Kubanov Kirill Mikhajlovich
Poretskov Anatolij Yurevich
Nesterov Oleg Nikolaevich
Gavrikov Viktor Nikolaevich
Sakhabutdinov Anas Gaptynurovich
description FIELD: chemistry.SUBSTANCE: method is done by dissolving the moist crumb butyl rubber in hydrocarbon solvents by filing a moist crumb rubber, solvent, the filing and withdrawal solution base polymer and water output in the hollow device. While the device has a zone of mixing, dissolving and settling in which the dissolution of rubber crumb, the solution circulation of base polymer, which is at the top of the unit, in the lower part of the zone and the zone of dissolution is held. Ratio of mixing zones of dissolution and zone equal to 3-4:1. When the mixing zone consists of two sections with different diameters, with the ratio of height to diameter of the upper site is -1 0.8:1, and the lower sector 0.3 -0.5:1.EFFECT: reducing losses and reaching base polymer averaging solution without spike concentration.1 dwg, 12 ex Изобретение относится к области получения галогенированных каучуков, конкретнее к способу приготовления базового полимера для производства галобутилкаучуков. Способ осуществляется путем растворения влажной крошки бутилового каучука в углеводородном растворителе путем подачи влажной крошки каучука, растворителя, подачи и вывода раствора базового полимера и вывода воды в полом аппарате. При этом аппарат имеет зоны смешения, растворения и отстоя, в котором растворение крошки каучука проводят циркуляцией раствора базового полимера, забираемого в верхней части аппарата, в нижние части зоны растворения и зоны смешения, причем соотношение объемов зоны растворения и зоны смешения равно 3-4:1. При этом зона смешения состоит из двух участков с разным диаметром, причем отношение высоты к диаметру верхнего участка составляет 0,8-1:1, а нижнего участка 0,3-0,5:1. Технический результат заключается в снижении потерь базового полимера и достижении усреднения раствора без резких скачков концентрации. 1 ил., 12 пр.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2620433C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2620433C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2620433C13</originalsourceid><addsrcrecordid>eNrjZPDwdQ3x8HdR8HdTCAhyDXAM8vRzV3ByDHZVCPD3ifR1DVII9vcJDfH091Nw8w8CqvF3CXUGqfFw9PF3Cg2J9FEICnVycg3iYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxQaFGZkYGJsbGzobGRCgBAMuFLM0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF PREPARING BASE POLYMER SOLUTION FOR PRODUCING HALOBUTYL RUBBER</title><source>esp@cenet</source><creator>Khabibullin Rafik Khatmullaevich ; Mironov Igor Vasilevich ; Aglyamov Irek Angamovich ; Sofronova Olga Vladimirovna ; Gazetdinov Ajdar Khanifovich ; Kubanov Kirill Mikhajlovich ; Poretskov Anatolij Yurevich ; Nesterov Oleg Nikolaevich ; Gavrikov Viktor Nikolaevich ; Sakhabutdinov Anas Gaptynurovich</creator><creatorcontrib>Khabibullin Rafik Khatmullaevich ; Mironov Igor Vasilevich ; Aglyamov Irek Angamovich ; Sofronova Olga Vladimirovna ; Gazetdinov Ajdar Khanifovich ; Kubanov Kirill Mikhajlovich ; Poretskov Anatolij Yurevich ; Nesterov Oleg Nikolaevich ; Gavrikov Viktor Nikolaevich ; Sakhabutdinov Anas Gaptynurovich</creatorcontrib><description>FIELD: chemistry.SUBSTANCE: method is done by dissolving the moist crumb butyl rubber in hydrocarbon solvents by filing a moist crumb rubber, solvent, the filing and withdrawal solution base polymer and water output in the hollow device. While the device has a zone of mixing, dissolving and settling in which the dissolution of rubber crumb, the solution circulation of base polymer, which is at the top of the unit, in the lower part of the zone and the zone of dissolution is held. Ratio of mixing zones of dissolution and zone equal to 3-4:1. When the mixing zone consists of two sections with different diameters, with the ratio of height to diameter of the upper site is -1 0.8:1, and the lower sector 0.3 -0.5:1.EFFECT: reducing losses and reaching base polymer averaging solution without spike concentration.1 dwg, 12 ex Изобретение относится к области получения галогенированных каучуков, конкретнее к способу приготовления базового полимера для производства галобутилкаучуков. Способ осуществляется путем растворения влажной крошки бутилового каучука в углеводородном растворителе путем подачи влажной крошки каучука, растворителя, подачи и вывода раствора базового полимера и вывода воды в полом аппарате. При этом аппарат имеет зоны смешения, растворения и отстоя, в котором растворение крошки каучука проводят циркуляцией раствора базового полимера, забираемого в верхней части аппарата, в нижние части зоны растворения и зоны смешения, причем соотношение объемов зоны растворения и зоны смешения равно 3-4:1. При этом зона смешения состоит из двух участков с разным диаметром, причем отношение высоты к диаметру верхнего участка составляет 0,8-1:1, а нижнего участка 0,3-0,5:1. Технический результат заключается в снижении потерь базового полимера и достижении усреднения раствора без резких скачков концентрации. 1 ил., 12 пр.</description><language>eng ; rus</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; GENERAL PROCESSES OF COMPOUNDING ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; WORKING-UP</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170525&amp;DB=EPODOC&amp;CC=RU&amp;NR=2620433C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170525&amp;DB=EPODOC&amp;CC=RU&amp;NR=2620433C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Khabibullin Rafik Khatmullaevich</creatorcontrib><creatorcontrib>Mironov Igor Vasilevich</creatorcontrib><creatorcontrib>Aglyamov Irek Angamovich</creatorcontrib><creatorcontrib>Sofronova Olga Vladimirovna</creatorcontrib><creatorcontrib>Gazetdinov Ajdar Khanifovich</creatorcontrib><creatorcontrib>Kubanov Kirill Mikhajlovich</creatorcontrib><creatorcontrib>Poretskov Anatolij Yurevich</creatorcontrib><creatorcontrib>Nesterov Oleg Nikolaevich</creatorcontrib><creatorcontrib>Gavrikov Viktor Nikolaevich</creatorcontrib><creatorcontrib>Sakhabutdinov Anas Gaptynurovich</creatorcontrib><title>METHOD OF PREPARING BASE POLYMER SOLUTION FOR PRODUCING HALOBUTYL RUBBER</title><description>FIELD: chemistry.SUBSTANCE: method is done by dissolving the moist crumb butyl rubber in hydrocarbon solvents by filing a moist crumb rubber, solvent, the filing and withdrawal solution base polymer and water output in the hollow device. While the device has a zone of mixing, dissolving and settling in which the dissolution of rubber crumb, the solution circulation of base polymer, which is at the top of the unit, in the lower part of the zone and the zone of dissolution is held. Ratio of mixing zones of dissolution and zone equal to 3-4:1. When the mixing zone consists of two sections with different diameters, with the ratio of height to diameter of the upper site is -1 0.8:1, and the lower sector 0.3 -0.5:1.EFFECT: reducing losses and reaching base polymer averaging solution without spike concentration.1 dwg, 12 ex Изобретение относится к области получения галогенированных каучуков, конкретнее к способу приготовления базового полимера для производства галобутилкаучуков. Способ осуществляется путем растворения влажной крошки бутилового каучука в углеводородном растворителе путем подачи влажной крошки каучука, растворителя, подачи и вывода раствора базового полимера и вывода воды в полом аппарате. При этом аппарат имеет зоны смешения, растворения и отстоя, в котором растворение крошки каучука проводят циркуляцией раствора базового полимера, забираемого в верхней части аппарата, в нижние части зоны растворения и зоны смешения, причем соотношение объемов зоны растворения и зоны смешения равно 3-4:1. При этом зона смешения состоит из двух участков с разным диаметром, причем отношение высоты к диаметру верхнего участка составляет 0,8-1:1, а нижнего участка 0,3-0,5:1. Технический результат заключается в снижении потерь базового полимера и достижении усреднения раствора без резких скачков концентрации. 1 ил., 12 пр.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPDwdQ3x8HdR8HdTCAhyDXAM8vRzV3ByDHZVCPD3ifR1DVII9vcJDfH091Nw8w8CqvF3CXUGqfFw9PF3Cg2J9FEICnVycg3iYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxQaFGZkYGJsbGzobGRCgBAMuFLM0</recordid><startdate>20170525</startdate><enddate>20170525</enddate><creator>Khabibullin Rafik Khatmullaevich</creator><creator>Mironov Igor Vasilevich</creator><creator>Aglyamov Irek Angamovich</creator><creator>Sofronova Olga Vladimirovna</creator><creator>Gazetdinov Ajdar Khanifovich</creator><creator>Kubanov Kirill Mikhajlovich</creator><creator>Poretskov Anatolij Yurevich</creator><creator>Nesterov Oleg Nikolaevich</creator><creator>Gavrikov Viktor Nikolaevich</creator><creator>Sakhabutdinov Anas Gaptynurovich</creator><scope>EVB</scope></search><sort><creationdate>20170525</creationdate><title>METHOD OF PREPARING BASE POLYMER SOLUTION FOR PRODUCING HALOBUTYL RUBBER</title><author>Khabibullin Rafik Khatmullaevich ; Mironov Igor Vasilevich ; Aglyamov Irek Angamovich ; Sofronova Olga Vladimirovna ; Gazetdinov Ajdar Khanifovich ; Kubanov Kirill Mikhajlovich ; Poretskov Anatolij Yurevich ; Nesterov Oleg Nikolaevich ; Gavrikov Viktor Nikolaevich ; Sakhabutdinov Anas Gaptynurovich</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2620433C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2017</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>Khabibullin Rafik Khatmullaevich</creatorcontrib><creatorcontrib>Mironov Igor Vasilevich</creatorcontrib><creatorcontrib>Aglyamov Irek Angamovich</creatorcontrib><creatorcontrib>Sofronova Olga Vladimirovna</creatorcontrib><creatorcontrib>Gazetdinov Ajdar Khanifovich</creatorcontrib><creatorcontrib>Kubanov Kirill Mikhajlovich</creatorcontrib><creatorcontrib>Poretskov Anatolij Yurevich</creatorcontrib><creatorcontrib>Nesterov Oleg Nikolaevich</creatorcontrib><creatorcontrib>Gavrikov Viktor Nikolaevich</creatorcontrib><creatorcontrib>Sakhabutdinov Anas Gaptynurovich</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Khabibullin Rafik Khatmullaevich</au><au>Mironov Igor Vasilevich</au><au>Aglyamov Irek Angamovich</au><au>Sofronova Olga Vladimirovna</au><au>Gazetdinov Ajdar Khanifovich</au><au>Kubanov Kirill Mikhajlovich</au><au>Poretskov Anatolij Yurevich</au><au>Nesterov Oleg Nikolaevich</au><au>Gavrikov Viktor Nikolaevich</au><au>Sakhabutdinov Anas Gaptynurovich</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF PREPARING BASE POLYMER SOLUTION FOR PRODUCING HALOBUTYL RUBBER</title><date>2017-05-25</date><risdate>2017</risdate><abstract>FIELD: chemistry.SUBSTANCE: method is done by dissolving the moist crumb butyl rubber in hydrocarbon solvents by filing a moist crumb rubber, solvent, the filing and withdrawal solution base polymer and water output in the hollow device. While the device has a zone of mixing, dissolving and settling in which the dissolution of rubber crumb, the solution circulation of base polymer, which is at the top of the unit, in the lower part of the zone and the zone of dissolution is held. Ratio of mixing zones of dissolution and zone equal to 3-4:1. When the mixing zone consists of two sections with different diameters, with the ratio of height to diameter of the upper site is -1 0.8:1, and the lower sector 0.3 -0.5:1.EFFECT: reducing losses and reaching base polymer averaging solution without spike concentration.1 dwg, 12 ex Изобретение относится к области получения галогенированных каучуков, конкретнее к способу приготовления базового полимера для производства галобутилкаучуков. Способ осуществляется путем растворения влажной крошки бутилового каучука в углеводородном растворителе путем подачи влажной крошки каучука, растворителя, подачи и вывода раствора базового полимера и вывода воды в полом аппарате. При этом аппарат имеет зоны смешения, растворения и отстоя, в котором растворение крошки каучука проводят циркуляцией раствора базового полимера, забираемого в верхней части аппарата, в нижние части зоны растворения и зоны смешения, причем соотношение объемов зоны растворения и зоны смешения равно 3-4:1. При этом зона смешения состоит из двух участков с разным диаметром, причем отношение высоты к диаметру верхнего участка составляет 0,8-1:1, а нижнего участка 0,3-0,5:1. Технический результат заключается в снижении потерь базового полимера и достижении усреднения раствора без резких скачков концентрации. 1 ил., 12 пр.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2620433C1
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
CHEMISTRY
COMPOSITIONS BASED THEREON
GENERAL PROCESSES OF COMPOUNDING
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
WORKING-UP
title METHOD OF PREPARING BASE POLYMER SOLUTION FOR PRODUCING HALOBUTYL RUBBER
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-06T14%3A58%3A00IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Khabibullin%20Rafik%20Khatmullaevich&rft.date=2017-05-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2620433C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true