METHOD OF FORMING LIGHT-ABSORBING COATING

FIELD: chemistry.SUBSTANCE: method includes preliminary chemical treatment of the initial surface of a component, electroplating with a nickel-phosphorus film and subsequent oxidation thereof in acidic solutions. The method enables to obtain a light-absorbing coating with a reflection coefficient of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NECHIPORENKO VIKTORIJA SERGEEVNA, KAZANTSEV OLEG JUR'EVICH, KOKIN EVGENIJ PETROVICH, MARUSEV DMITRIJ VADIMOVICH, VIGOVSKAJA TAT'JANA VLADIMIROVNA, L'VOVA NATALIJA MIKHAJLOVNA, SURIN JURIJ VASIL'EVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: chemistry.SUBSTANCE: method includes preliminary chemical treatment of the initial surface of a component, electroplating with a nickel-phosphorus film and subsequent oxidation thereof in acidic solutions. The method enables to obtain a light-absorbing coating with a reflection coefficient of not more than 0.5% in a spectral wavelength range of 250-2000 nm and not more than 0.8% in the 2000-2500 nm range.EFFECT: improved output characteristics of optical systems.3 dwg Изобретение относится к области технологии формирования светопоглощающих покрытий методом гальванического осаждения никель-фосфорных пленок и может применяться для чернения конструкционных деталей оптических информационных систем для подавления рассеянного излучения и улучшения выходных характеристик оптических систем. Способ включает предварительную химическую обработку исходной поверхности детали, гальваническое осаждение никель-фосфорной пленки и последующее ее оксидирование в кислотных растворах. Способ позволяет получить светопоглощающее покрытие с коэффициентом отражения не более 0,5% в спектральном диапазоне длин волн 250-2000 нм и не превышающим 0,8% в диапазоне 2000-2500 нм. 3 ил.