METHOD OF STEEL MICROALLOYING BY BORON
FIELD: metallurgy.SUBSTANCE: steel microalloying by boron is performed at output by the addition to the ladle of the aluminium and complex alloy of ferrosilicon boron in amount of 4.0-7.5 kg/t of steel with ratio of aluminium to ferrosilicon boron within range (0.25-0.50), at that the ferrosilicon b...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: metallurgy.SUBSTANCE: steel microalloying by boron is performed at output by the addition to the ladle of the aluminium and complex alloy of ferrosilicon boron in amount of 4.0-7.5 kg/t of steel with ratio of aluminium to ferrosilicon boron within range (0.25-0.50), at that the ferrosilicon boron contains in wt %: 60-65 Si and 0.5-2.0 B.EFFECT: reduced expenses for metal production, reduced time of out of furnace treatment at ladle-furnace unit, and increased quality of the metal products.2 cl, 1 tbl
Изобретение относится к области черной металлургии и может быть использовано для совершенствования технологии микролегирования стали бором. Микролегирование стали бором осуществляют на выпуске присадкой в ковш алюминия и комплексного сплава ферросиликобора в количестве 4,0-7,5 кг/т стали с отношением алюминия к ферросиликобору в пределах (0,25-0,50), при этом ферросиликобор содержит, мас.%: 60-65 Si и 0,5-2,0 В. Изобретение позволяет снизить затраты на производство металла, сократить время внепечной обработки на установке ковш-печь и повысить качество металлопродукции. 1 з.п. ф-лы, 1 табл. |
---|