METHOD OF OBTAINING CeO-SnO- BASED CATALYST ON FIBREGLASS CARRIER

FIELD: chemistry.SUBSTANCE: method includes preparation of carrier by thermal processing at 500°C, application of alcohol film-generating solution by method of stretching at rate 100 mm/min, drying at 60°C for 1 h and annealing at 750°C for 4 h. Film-generating solution is applied on fibreglass carr...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GALANOV SERGEJ IVANOVICH, KUZNETSOVA SVETLANA ANATOLEVNA, KOZIK VLADIMIR VASILEVICH, KHALIPOVA OLGA SERGEEVNA
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GALANOV SERGEJ IVANOVICH
KUZNETSOVA SVETLANA ANATOLEVNA
KOZIK VLADIMIR VASILEVICH
KHALIPOVA OLGA SERGEEVNA
description FIELD: chemistry.SUBSTANCE: method includes preparation of carrier by thermal processing at 500°C, application of alcohol film-generating solution by method of stretching at rate 100 mm/min, drying at 60°C for 1 h and annealing at 750°C for 4 h. Film-generating solution is applied on fibreglass carrier by method of soaking with further drying at 60°C for 1 h and annealing at 600-750°C for 1 h. Catalyst, which is obtained in form of cloth, is cut at output in accordance with reactor shape and packed in layers at angle of 20-30°, with formation of honeycomb structure, with the following component ratio in film-generating solution, wt %: Ce(NO)·6HO - from 6.0 to 12.0, SnCl·5HO - from 16.6 to 22.3, CHOHCOOH - from 9.1 to 10.0, 96%-by weight CHOH - the remaining part.EFFECT: method makes it possible to obtain catalysts, characterised by high permeability of gas mixture flow.2 dwg, 4 ex Изобретение относится к способу получения катализатора на основе CeO-SnОна стеклотканном носителе. Данный способ включает подготовку носителя путем термической обработки при 500°С, нанесение спиртового пленкообразующего раствора методом вытягивания со скоростью 100 мм/мин, сушку при 60°С 1 ч и отжиг при 750°С 4 ч. При этом пленкообразующий раствор наносится на стеклотканный носитель методом пропитки с последующей сушкой при 60°С 1 ч и отжигом при 600-750°С 1 ч. Полученный в виде полотна катализатор на выходе обрезается согласно форме реактора и упаковывается слоями под углом 20-30°, формируя структуру сот, при следующем соотношении компонентов в пленкообразующем растворе, мас.%: Сe(NO)·6HO - от 6,0 до 12,0, SnCl·5HO - от 16,6 до 22,3, СНOHCOOH - от 9,1 до 10,0, 96%-ный по массе СНOH - остальное. Предлагаемый способ позволяет получать катализаторы, характеризующиеся высокой проницаемостью потока газовой смеси. 2 ил., 4 пр.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2554943C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2554943C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2554943C13</originalsourceid><addsrcrecordid>eNrjZHD0dQ3x8HdR8HdT8HcKcfT08_RzV3BO9dcNzvPXVXByDHZ1UXB2DHH0iQwOUfD3U3DzdApydfdxDA4GCgcFeboG8TCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQI1NTE0sTY2dDYyKUAAB1IiqV</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF OBTAINING CeO-SnO- BASED CATALYST ON FIBREGLASS CARRIER</title><source>esp@cenet</source><creator>GALANOV SERGEJ IVANOVICH ; KUZNETSOVA SVETLANA ANATOLEVNA ; KOZIK VLADIMIR VASILEVICH ; KHALIPOVA OLGA SERGEEVNA</creator><creatorcontrib>GALANOV SERGEJ IVANOVICH ; KUZNETSOVA SVETLANA ANATOLEVNA ; KOZIK VLADIMIR VASILEVICH ; KHALIPOVA OLGA SERGEEVNA</creatorcontrib><description>FIELD: chemistry.SUBSTANCE: method includes preparation of carrier by thermal processing at 500°C, application of alcohol film-generating solution by method of stretching at rate 100 mm/min, drying at 60°C for 1 h and annealing at 750°C for 4 h. Film-generating solution is applied on fibreglass carrier by method of soaking with further drying at 60°C for 1 h and annealing at 600-750°C for 1 h. Catalyst, which is obtained in form of cloth, is cut at output in accordance with reactor shape and packed in layers at angle of 20-30°, with formation of honeycomb structure, with the following component ratio in film-generating solution, wt %: Ce(NO)·6HO - from 6.0 to 12.0, SnCl·5HO - from 16.6 to 22.3, CHOHCOOH - from 9.1 to 10.0, 96%-by weight CHOH - the remaining part.EFFECT: method makes it possible to obtain catalysts, characterised by high permeability of gas mixture flow.2 dwg, 4 ex Изобретение относится к способу получения катализатора на основе CeO-SnОна стеклотканном носителе. Данный способ включает подготовку носителя путем термической обработки при 500°С, нанесение спиртового пленкообразующего раствора методом вытягивания со скоростью 100 мм/мин, сушку при 60°С 1 ч и отжиг при 750°С 4 ч. При этом пленкообразующий раствор наносится на стеклотканный носитель методом пропитки с последующей сушкой при 60°С 1 ч и отжигом при 600-750°С 1 ч. Полученный в виде полотна катализатор на выходе обрезается согласно форме реактора и упаковывается слоями под углом 20-30°, формируя структуру сот, при следующем соотношении компонентов в пленкообразующем растворе, мас.%: Сe(NO)·6HO - от 6,0 до 12,0, SnCl·5HO - от 16,6 до 22,3, СНOHCOOH - от 9,1 до 10,0, 96%-ный по массе СНOH - остальное. Предлагаемый способ позволяет получать катализаторы, характеризующиеся высокой проницаемостью потока газовой смеси. 2 ил., 4 пр.</description><language>eng ; rus</language><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; THEIR RELEVANT APPARATUS ; TRANSPORTING</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150710&amp;DB=EPODOC&amp;CC=RU&amp;NR=2554943C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150710&amp;DB=EPODOC&amp;CC=RU&amp;NR=2554943C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GALANOV SERGEJ IVANOVICH</creatorcontrib><creatorcontrib>KUZNETSOVA SVETLANA ANATOLEVNA</creatorcontrib><creatorcontrib>KOZIK VLADIMIR VASILEVICH</creatorcontrib><creatorcontrib>KHALIPOVA OLGA SERGEEVNA</creatorcontrib><title>METHOD OF OBTAINING CeO-SnO- BASED CATALYST ON FIBREGLASS CARRIER</title><description>FIELD: chemistry.SUBSTANCE: method includes preparation of carrier by thermal processing at 500°C, application of alcohol film-generating solution by method of stretching at rate 100 mm/min, drying at 60°C for 1 h and annealing at 750°C for 4 h. Film-generating solution is applied on fibreglass carrier by method of soaking with further drying at 60°C for 1 h and annealing at 600-750°C for 1 h. Catalyst, which is obtained in form of cloth, is cut at output in accordance with reactor shape and packed in layers at angle of 20-30°, with formation of honeycomb structure, with the following component ratio in film-generating solution, wt %: Ce(NO)·6HO - from 6.0 to 12.0, SnCl·5HO - from 16.6 to 22.3, CHOHCOOH - from 9.1 to 10.0, 96%-by weight CHOH - the remaining part.EFFECT: method makes it possible to obtain catalysts, characterised by high permeability of gas mixture flow.2 dwg, 4 ex Изобретение относится к способу получения катализатора на основе CeO-SnОна стеклотканном носителе. Данный способ включает подготовку носителя путем термической обработки при 500°С, нанесение спиртового пленкообразующего раствора методом вытягивания со скоростью 100 мм/мин, сушку при 60°С 1 ч и отжиг при 750°С 4 ч. При этом пленкообразующий раствор наносится на стеклотканный носитель методом пропитки с последующей сушкой при 60°С 1 ч и отжигом при 600-750°С 1 ч. Полученный в виде полотна катализатор на выходе обрезается согласно форме реактора и упаковывается слоями под углом 20-30°, формируя структуру сот, при следующем соотношении компонентов в пленкообразующем растворе, мас.%: Сe(NO)·6HO - от 6,0 до 12,0, SnCl·5HO - от 16,6 до 22,3, СНOHCOOH - от 9,1 до 10,0, 96%-ный по массе СНOH - остальное. Предлагаемый способ позволяет получать катализаторы, характеризующиеся высокой проницаемостью потока газовой смеси. 2 ил., 4 пр.</description><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD0dQ3x8HdR8HdT8HcKcfT08_RzV3BO9dcNzvPXVXByDHZ1UXB2DHH0iQwOUfD3U3DzdApydfdxDA4GCgcFeboG8TCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQI1NTE0sTY2dDYyKUAAB1IiqV</recordid><startdate>20150710</startdate><enddate>20150710</enddate><creator>GALANOV SERGEJ IVANOVICH</creator><creator>KUZNETSOVA SVETLANA ANATOLEVNA</creator><creator>KOZIK VLADIMIR VASILEVICH</creator><creator>KHALIPOVA OLGA SERGEEVNA</creator><scope>EVB</scope></search><sort><creationdate>20150710</creationdate><title>METHOD OF OBTAINING CeO-SnO- BASED CATALYST ON FIBREGLASS CARRIER</title><author>GALANOV SERGEJ IVANOVICH ; KUZNETSOVA SVETLANA ANATOLEVNA ; KOZIK VLADIMIR VASILEVICH ; KHALIPOVA OLGA SERGEEVNA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2554943C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2015</creationdate><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>GALANOV SERGEJ IVANOVICH</creatorcontrib><creatorcontrib>KUZNETSOVA SVETLANA ANATOLEVNA</creatorcontrib><creatorcontrib>KOZIK VLADIMIR VASILEVICH</creatorcontrib><creatorcontrib>KHALIPOVA OLGA SERGEEVNA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GALANOV SERGEJ IVANOVICH</au><au>KUZNETSOVA SVETLANA ANATOLEVNA</au><au>KOZIK VLADIMIR VASILEVICH</au><au>KHALIPOVA OLGA SERGEEVNA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF OBTAINING CeO-SnO- BASED CATALYST ON FIBREGLASS CARRIER</title><date>2015-07-10</date><risdate>2015</risdate><abstract>FIELD: chemistry.SUBSTANCE: method includes preparation of carrier by thermal processing at 500°C, application of alcohol film-generating solution by method of stretching at rate 100 mm/min, drying at 60°C for 1 h and annealing at 750°C for 4 h. Film-generating solution is applied on fibreglass carrier by method of soaking with further drying at 60°C for 1 h and annealing at 600-750°C for 1 h. Catalyst, which is obtained in form of cloth, is cut at output in accordance with reactor shape and packed in layers at angle of 20-30°, with formation of honeycomb structure, with the following component ratio in film-generating solution, wt %: Ce(NO)·6HO - from 6.0 to 12.0, SnCl·5HO - from 16.6 to 22.3, CHOHCOOH - from 9.1 to 10.0, 96%-by weight CHOH - the remaining part.EFFECT: method makes it possible to obtain catalysts, characterised by high permeability of gas mixture flow.2 dwg, 4 ex Изобретение относится к способу получения катализатора на основе CeO-SnОна стеклотканном носителе. Данный способ включает подготовку носителя путем термической обработки при 500°С, нанесение спиртового пленкообразующего раствора методом вытягивания со скоростью 100 мм/мин, сушку при 60°С 1 ч и отжиг при 750°С 4 ч. При этом пленкообразующий раствор наносится на стеклотканный носитель методом пропитки с последующей сушкой при 60°С 1 ч и отжигом при 600-750°С 1 ч. Полученный в виде полотна катализатор на выходе обрезается согласно форме реактора и упаковывается слоями под углом 20-30°, формируя структуру сот, при следующем соотношении компонентов в пленкообразующем растворе, мас.%: Сe(NO)·6HO - от 6,0 до 12,0, SnCl·5HO - от 16,6 до 22,3, СНOHCOOH - от 9,1 до 10,0, 96%-ный по массе СНOH - остальное. Предлагаемый способ позволяет получать катализаторы, характеризующиеся высокой проницаемостью потока газовой смеси. 2 ил., 4 пр.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2554943C1
source esp@cenet
subjects CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
THEIR RELEVANT APPARATUS
TRANSPORTING
title METHOD OF OBTAINING CeO-SnO- BASED CATALYST ON FIBREGLASS CARRIER
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T10%3A13%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GALANOV%20SERGEJ%20IVANOVICH&rft.date=2015-07-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2554943C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true