METHOD OF OBTAINING OF HYDROPHOBIC ADDITIVE FOR BITUMEN CONCRETE MIX AND THE METHOD OF OBTAINING BITUMEN CONCRETE MIX WITH ITS USE

FIELD: construction.SUBSTANCE: in the method of obtaining a hydrophobic additive for bitumen concrete mix which comprises mixing of oily slime with unslaked lime and the subsequent adding of a heated component, thorough mixing within 20 min. maximum with the subsequent unloading of the obtained gran...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FLISJUK OLEG MIKHAJLOVICH, KONSTANTINOV VALERIJ ANATOL'EVICH, MURATOV OLEG VADIMOVICH, BORISOVA EKATERINA IGOREVNA, SHININOV TIMUR NIKOLAEVICH, MAJDANOVA NATALIJA VASIL'EVNA, KRUKOVSKIJ OLEG NIKOLAEVICH, URCHEVA JULIJA ALEKSANDROVNA, SYROEZHKO ALEKSANDR MIKHAJLOVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: construction.SUBSTANCE: in the method of obtaining a hydrophobic additive for bitumen concrete mix which comprises mixing of oily slime with unslaked lime and the subsequent adding of a heated component, thorough mixing within 20 min. maximum with the subsequent unloading of the obtained granulated product, pre-dehydrated oil slime is used, which contain no more than 20% by weight of hydrocarbons and up to 10% by weight of water, where unslaked lime is added at their ratio 1:0.1-0.2 from the weight of the dehydrated mix, after mixing and obtaining of the uniform mix heated up to the temperature 70°C, the obtained mix is loaded into the high-speed granulator with the rotating rotor fitted with pins for material mixing heated up to the temperature 110-130°C the pre-heated road bitumen is added as a component at the temperature 120-150°C amounting 10-15% of the loaded mix weight, the mixing is conducted at the rotor rotation frequency 500 rpm and the linear speed of the rotor pins 6.5 m/s, therefore the granulated hydrophobic additive is obtained. The method of obtaining of bitumen concrete mix which is characterized by mixing of mixed ingredients heated granite macadam with the fraction up to 5 mm mixed with granite dust, bitumen and a hydrophobic additive named above, and the ration of mixed ingredients amounts: granite macadam with the fraction up to 5 mm mixed with granite dust, the granulated hydrophobic additive and bitumen amounts, %: (88-89):(6-6.5):(5-5.5).EFFECT: improvement of hydrophobic properties.2 cl, 6 ex Изобретение относится к области получения товарных продуктов, а именно - гидрофобной добавки для асфальтобетонных смесей и асфальтобетонной смеси с ее использованием. В способе получения гидрофобной добавки в асфальтобетонную смесь, включающем смешение нефтесодержащего шлама с негашеной известью и последующее введение нагретого компонента, интенсивное перемешивание в течение не более 20 мин с последующей выгрузкой полученного гранулированного продукта, используют нефтяной шлам, предварительно обезвоженный, содержащий не более 20 мас. % углеводородов и до 10 мас. % воды, к которому добавляют негашеную известь при их соотношении 1:0,1-0,2 от массы обезвоженной смеси, после перемешивания и получения однородной смеси, разогревшейся до температуры 70°C, полученную смесь загружают в скоростной гранулятор с вращающимся ротором, снабженным пальцами для перемешивания материала, разогретый до температуры 110-130°C, добавляют в качестве предварит