METHOD OF GLASS-PRODUCT BENDING
FIELD: chemistry.SUBSTANCE: glass-blank is placed on a mould with a specified curvature of the moulding surface and glass heating is realised. In the process of heating, when the temperature of 450-550°C is reached, additional heaters are turned on, which realise controlled heating of areas of the g...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: chemistry.SUBSTANCE: glass-blank is placed on a mould with a specified curvature of the moulding surface and glass heating is realised. In the process of heating, when the temperature of 450-550°C is reached, additional heaters are turned on, which realise controlled heating of areas of the glass open surface due to the vertical movement of the heaters and an independent change of power of each of heat irradiators.EFFECT: increase of the curve precision.2 cl, 3 dwg
Изобретение относится к моллированию листового стекла. Технический результат изобретения заключается в повышении точности изгиба. Стеклозаготовку размещают на форме с заданной кривизной формующей поверхности и осуществляют нагрев стекла. В процессе нагрева при достижении температуры 450-550°C включают дополнительные нагреватели, осуществляющие управляемый подогрев участков открытой поверхности стекла за счет вертикального перемещения нагревателей и независимого изменения мощности каждого из тепловых излучателей. 1 з.п. ф-лы, 3 ил. |
---|