METHOD OF PLOUGH SHARE HARDENING

FIELD: metallurgy.SUBSTANCE: plough surface is subjected to electromechanical treatment at current density of up to 10A/mto make hardened zones deep to 3 mm shaped to continuous lines. Front and bottom blades are hardened as well as plough tip at 20-40 mm from front blade with hardened zone width of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JAKOVLEV SERGEJ ALEKSANDROVICH, JAKOVLEVA IRINA GENNAD'EVNA
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: metallurgy.SUBSTANCE: plough surface is subjected to electromechanical treatment at current density of up to 10A/mto make hardened zones deep to 3 mm shaped to continuous lines. Front and bottom blades are hardened as well as plough tip at 20-40 mm from front blade with hardened zone width of 10-20 mm.EFFECT: longer life owing to higher strength, wear resistance and self-sharpening.1 dwg Изобретение может быть использовано для поверхностного упрочнения лемехов плугов сельскохозяйственных машин. Осуществляют электромеханическую обработку поверхности лемеха при плотности тока до 10А/мс образованием упрочненных зон глубиной до 3 мм в виде непрерывных линий. Упрочнению подвергают переднее и нижнее лезвие, а также носок лемеха на расстоянии 20...40 мм от переднего лезвия с шириной упрочненной зоны 10...20 мм. Техническим результатом изобретения является повышение долговечности лемехов за счет улучшения их прочностных характеристик, износостойкости к абразивному износу и способности к самозатачиванию. 1 ил.