SOLUTION FOR CHEMICAL DEPOSITION OF COMPOSITE COATING
FIELD: chemistry. ^ SUBSTANCE: solution for chemical deposition of composite coating contains the following components, g/l: nickel sulphate 10-30, sodium hypophosphite 10-20, sodium acetate 10-15, polyvinyl alcohol 0.5-1, nanofibre 0.1-10, distilled water - 1 litre. The nanofibre is added to the so...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: chemistry. ^ SUBSTANCE: solution for chemical deposition of composite coating contains the following components, g/l: nickel sulphate 10-30, sodium hypophosphite 10-20, sodium acetate 10-15, polyvinyl alcohol 0.5-1, nanofibre 0.1-10, distilled water - 1 litre. The nanofibre is added to the solution in form of powder particles of aluminium oxide-hydroxide phases with particle size 100-700 nm. ^ EFFECT: invention enables to obtain a composite coating, having low coefficient of friction, high wear resistance and high corrosion resistance. ^ 1 tbl, 1 ex
Изобретение относится к нанесению покрытий на металлические изделия, в частности к получению композиционного покрытия на металлических изделиях методом химического осаждения. Раствор для химического осаждения композиционного покрытия содержит следующие компоненты, г/л: никель сернокислый 10-30, натрия гипофосфит 10-20, натрий уксуснокислый 10-15, спирт поливиниловый 0,5-1, нановолокно 0,1-10, дистиллированная вода 1 литр. При этом нановолокно вводят в раствор в виде частиц порошка оксидно-гидроксидных фаз алюминия с размерностью 100-700 нм. Изобретение позволяет получить композиционное покрытие, обладающее низким коэффициентом трения, высокой износостойкостью и высокой коррозионной стойкостью. 1 табл., 1 пр. |
---|