METHOD TO GLUE TIMBER-BASED MATERIALS
FIELD: construction. ^ SUBSTANCE: surfaces to be glued are coated with a synthetic glue KFZh based on an aminoformaldehyde resin. These surfaces are joined. Adhered parts are placed between DC poles of an electromagnet so that magnetic force lines are directed perpendicularly to an adhesive seam wit...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: construction. ^ SUBSTANCE: surfaces to be glued are coated with a synthetic glue KFZh based on an aminoformaldehyde resin. These surfaces are joined. Adhered parts are placed between DC poles of an electromagnet so that magnetic force lines are directed perpendicularly to an adhesive seam with intensity of (3-24)ù104 A/m. The glue as an acid hardener contains a chemical production waste, containing at least 80% maleic acid in amount from 0.5 to 2.0 wt parts per 100 wt parts of the aminoformaldehyde resin. ^ EFFECT: invention makes it possible to increase strength indices of glue joints. ^ 1 tbl, 1 ex
Изобретение относится к технологии получения клеевых соединений и может быть использовано в строительной и деревообрабатывающей промышленности при изготовлении клееных материалов. На поверхности, подлежащие склеиванию, наносят синтетический клей КФЖ на основе карбамидоформальдегидной смолы. Соединяют эти поверхности. Склеиваемые детали помещают между полюсами постоянного тока электромагнита таким образом, чтобы магнитные силовые линии были направлены перпендикулярно клеевому шву с напряженностью (3-24)×104 А/м. Клей в качестве кислотного отвердителя содержит отход химического производства, содержащий не менее 80% малеиновой кислоты в количестве от 0,5 до 2,0 мас.ч. на 100 мас.ч. карбамидоформальдегидной смолы. Изобретение позволяет повысить прочностные показатели клеевых соединений. 1 табл. |
---|