METHOD OF PRODUCING BISMUTH (III) OXIDE POWDER

FIELD: chemistry. ^ SUBSTANCE: bismuth metal is loaded into a tubular quartz reactor and heated until the metal is completely molten. The reactor is rotated and the molten mass is treated in a reducing atmosphere which is a mixture of hydrogen or ethanol with an inert gas in order to remove the oxid...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BYZOV GRIGORIJ PETROVICH, NOVOSELOV IGOR' IVANOVICH, SHUBIN JURIJ VIKTOROVICH, MAKAROV IGOR' VASIL'EVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: chemistry. ^ SUBSTANCE: bismuth metal is loaded into a tubular quartz reactor and heated until the metal is completely molten. The reactor is rotated and the molten mass is treated in a reducing atmosphere which is a mixture of hydrogen or ethanol with an inert gas in order to remove the oxide film from the surface of the metal. Bismuth is then oxidised with oxygen at 350C and rate of supply of oxygen of 30 l/h. ^ EFFECT: invention enables obtaining fine high-purity powder of bismuth oxide with high output and having particle size less than 150 mcm. ^ 2 cl, 1 ex Изобретение может быть использовано в химической технологии. Металлический висмут загружают в трубчатый кварцевый реактор и нагревают до полного расплавления металла. Включают вращение реактора и обрабатывают расплав в восстановительной атмосфере, представляющей собой смесь водорода или этилового спирта с инертным газом с целью удаления с поверхности металла оксидной пленки. Затем проводят окисление висмута кислородом при 350°С и скорости подачи кислорода 30 л/ч. Изобретение позволяет получить мелкодисперсный высокочистый порошок оксида висмута (III) с выходом до 95% и преобладающим размером частиц менее 150 мкм. 1 з.п ф-лы.