METHOD FOR PRODUCTION OF SYNTHETIC TECHNICAL CLOTH EDGE

FIELD: technological processes. ^ SUBSTANCE: edge of cloth consists of reinforced structure adjacent to solder and made of web threads and polypropylene binder. Web is thermally shrunk, cut along its width by a cutting tool with a temperature of 450-650C to make a solder and introduction of polymer...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GUSAKOV ALEKSANDR VASIL'EVICH, NADTOCHEEVA VALENTINA MAKSIMOVNA, ROMANOVA ANNA NIKOLAEVNA, NIKITINA IRINA VALENTINOVNA
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GUSAKOV ALEKSANDR VASIL'EVICH
NADTOCHEEVA VALENTINA MAKSIMOVNA
ROMANOVA ANNA NIKOLAEVNA
NIKITINA IRINA VALENTINOVNA
description FIELD: technological processes. ^ SUBSTANCE: edge of cloth consists of reinforced structure adjacent to solder and made of web threads and polypropylene binder. Web is thermally shrunk, cut along its width by a cutting tool with a temperature of 450-650C to make a solder and introduction of polymer binder melt from upper and lower sides of web. Melt is supplied under pressure from extruder. As polymer binder they use polypropylene with index of melt fluidity of 0.6-15. Amount of polymer applied per unit of web length is defined depending on thickness of web, surface density, width of edge, total number of main and weft thread types, from which the web is woven, density of material thread, weight portion of thread in web, volume shrinkage of melt and density of polypropylene. ^ EFFECT: improved mechanical and hydrolytic stability at high temperatures in atmosphere of high humidity, and resistance to side impact and abrasive loads. ^ 3 cl, 1 dwg, 3 tbl Изобретение относится к способу получения кромок синтетических технических полотен, в частности сушильных сеток бумаго- и картоноделательных машин. Кромка полотна состоит из примыкающей к припаю армированной структуры из нитей сетки и полипропиленового связующего. Осуществляют термоусадку сетки, обрезание ее по ширине режущим инструментом с температурой 450-650°С с образованием припая и внесение с верхней и нижней сторон сетки расплава полимерного связующего. Расплав поступает под давлением из экструдера. В качестве полимерного связующего используют полипропилен с индексом текучести расплава 0,6-15. Количество наносимого на единицу длины полотна полимера определяют в зависимости от толщины сетки, поверхностной плотности, ширины кромки, общего числа видов основных и уточных нитей, из которых соткана сетка, плотности материала нити, массовой доли нити в сетке, объемной усадки расплава и плотности полипропилена. Кромка, полученная данным способом, обладает увеличенной механической и гидролитической устойчивостью при температурах выше 100°С в атмосфере высокой влажности, а также сопротивлением к боковым ударным и абразивным нагрузкам. 2 з.п. ф-лы, 1 ил., 3 табл.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2371534C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2371534C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2371534C13</originalsourceid><addsrcrecordid>eNrjZDD3dQ3x8HdRcPMPUggI8ncJdQ7x9PdT8HdTCI70C_FwDfF0Vghxdfbw83R29FFw9vEP8VBwdXF35WFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8UGhRsbmhqbGJs6GxkQoAQDt8ifZ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCTION OF SYNTHETIC TECHNICAL CLOTH EDGE</title><source>esp@cenet</source><creator>GUSAKOV ALEKSANDR VASIL'EVICH ; NADTOCHEEVA VALENTINA MAKSIMOVNA ; ROMANOVA ANNA NIKOLAEVNA ; NIKITINA IRINA VALENTINOVNA</creator><creatorcontrib>GUSAKOV ALEKSANDR VASIL'EVICH ; NADTOCHEEVA VALENTINA MAKSIMOVNA ; ROMANOVA ANNA NIKOLAEVNA ; NIKITINA IRINA VALENTINOVNA</creatorcontrib><description>FIELD: technological processes. ^ SUBSTANCE: edge of cloth consists of reinforced structure adjacent to solder and made of web threads and polypropylene binder. Web is thermally shrunk, cut along its width by a cutting tool with a temperature of 450-650C to make a solder and introduction of polymer binder melt from upper and lower sides of web. Melt is supplied under pressure from extruder. As polymer binder they use polypropylene with index of melt fluidity of 0.6-15. Amount of polymer applied per unit of web length is defined depending on thickness of web, surface density, width of edge, total number of main and weft thread types, from which the web is woven, density of material thread, weight portion of thread in web, volume shrinkage of melt and density of polypropylene. ^ EFFECT: improved mechanical and hydrolytic stability at high temperatures in atmosphere of high humidity, and resistance to side impact and abrasive loads. ^ 3 cl, 1 dwg, 3 tbl Изобретение относится к способу получения кромок синтетических технических полотен, в частности сушильных сеток бумаго- и картоноделательных машин. Кромка полотна состоит из примыкающей к припаю армированной структуры из нитей сетки и полипропиленового связующего. Осуществляют термоусадку сетки, обрезание ее по ширине режущим инструментом с температурой 450-650°С с образованием припая и внесение с верхней и нижней сторон сетки расплава полимерного связующего. Расплав поступает под давлением из экструдера. В качестве полимерного связующего используют полипропилен с индексом текучести расплава 0,6-15. Количество наносимого на единицу длины полотна полимера определяют в зависимости от толщины сетки, поверхностной плотности, ширины кромки, общего числа видов основных и уточных нитей, из которых соткана сетка, плотности материала нити, массовой доли нити в сетке, объемной усадки расплава и плотности полипропилена. Кромка, полученная данным способом, обладает увеличенной механической и гидролитической устойчивостью при температурах выше 100°С в атмосфере высокой влажности, а также сопротивлением к боковым ударным и абразивным нагрузкам. 2 з.п. ф-лы, 1 ил., 3 табл.</description><language>eng ; rus</language><subject>METHODS OF PRODUCING PAPER THEREON ; PAPER-MAKING ; PAPER-MAKING MACHINES ; PRODUCTION OF CELLULOSE ; TEXTILES</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20091027&amp;DB=EPODOC&amp;CC=RU&amp;NR=2371534C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20091027&amp;DB=EPODOC&amp;CC=RU&amp;NR=2371534C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GUSAKOV ALEKSANDR VASIL'EVICH</creatorcontrib><creatorcontrib>NADTOCHEEVA VALENTINA MAKSIMOVNA</creatorcontrib><creatorcontrib>ROMANOVA ANNA NIKOLAEVNA</creatorcontrib><creatorcontrib>NIKITINA IRINA VALENTINOVNA</creatorcontrib><title>METHOD FOR PRODUCTION OF SYNTHETIC TECHNICAL CLOTH EDGE</title><description>FIELD: technological processes. ^ SUBSTANCE: edge of cloth consists of reinforced structure adjacent to solder and made of web threads and polypropylene binder. Web is thermally shrunk, cut along its width by a cutting tool with a temperature of 450-650C to make a solder and introduction of polymer binder melt from upper and lower sides of web. Melt is supplied under pressure from extruder. As polymer binder they use polypropylene with index of melt fluidity of 0.6-15. Amount of polymer applied per unit of web length is defined depending on thickness of web, surface density, width of edge, total number of main and weft thread types, from which the web is woven, density of material thread, weight portion of thread in web, volume shrinkage of melt and density of polypropylene. ^ EFFECT: improved mechanical and hydrolytic stability at high temperatures in atmosphere of high humidity, and resistance to side impact and abrasive loads. ^ 3 cl, 1 dwg, 3 tbl Изобретение относится к способу получения кромок синтетических технических полотен, в частности сушильных сеток бумаго- и картоноделательных машин. Кромка полотна состоит из примыкающей к припаю армированной структуры из нитей сетки и полипропиленового связующего. Осуществляют термоусадку сетки, обрезание ее по ширине режущим инструментом с температурой 450-650°С с образованием припая и внесение с верхней и нижней сторон сетки расплава полимерного связующего. Расплав поступает под давлением из экструдера. В качестве полимерного связующего используют полипропилен с индексом текучести расплава 0,6-15. Количество наносимого на единицу длины полотна полимера определяют в зависимости от толщины сетки, поверхностной плотности, ширины кромки, общего числа видов основных и уточных нитей, из которых соткана сетка, плотности материала нити, массовой доли нити в сетке, объемной усадки расплава и плотности полипропилена. Кромка, полученная данным способом, обладает увеличенной механической и гидролитической устойчивостью при температурах выше 100°С в атмосфере высокой влажности, а также сопротивлением к боковым ударным и абразивным нагрузкам. 2 з.п. ф-лы, 1 ил., 3 табл.</description><subject>METHODS OF PRODUCING PAPER THEREON</subject><subject>PAPER-MAKING</subject><subject>PAPER-MAKING MACHINES</subject><subject>PRODUCTION OF CELLULOSE</subject><subject>TEXTILES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD3dQ3x8HdRcPMPUggI8ncJdQ7x9PdT8HdTCI70C_FwDfF0Vghxdfbw83R29FFw9vEP8VBwdXF35WFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8UGhRsbmhqbGJs6GxkQoAQDt8ifZ</recordid><startdate>20091027</startdate><enddate>20091027</enddate><creator>GUSAKOV ALEKSANDR VASIL'EVICH</creator><creator>NADTOCHEEVA VALENTINA MAKSIMOVNA</creator><creator>ROMANOVA ANNA NIKOLAEVNA</creator><creator>NIKITINA IRINA VALENTINOVNA</creator><scope>EVB</scope></search><sort><creationdate>20091027</creationdate><title>METHOD FOR PRODUCTION OF SYNTHETIC TECHNICAL CLOTH EDGE</title><author>GUSAKOV ALEKSANDR VASIL'EVICH ; NADTOCHEEVA VALENTINA MAKSIMOVNA ; ROMANOVA ANNA NIKOLAEVNA ; NIKITINA IRINA VALENTINOVNA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2371534C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2009</creationdate><topic>METHODS OF PRODUCING PAPER THEREON</topic><topic>PAPER-MAKING</topic><topic>PAPER-MAKING MACHINES</topic><topic>PRODUCTION OF CELLULOSE</topic><topic>TEXTILES</topic><toplevel>online_resources</toplevel><creatorcontrib>GUSAKOV ALEKSANDR VASIL'EVICH</creatorcontrib><creatorcontrib>NADTOCHEEVA VALENTINA MAKSIMOVNA</creatorcontrib><creatorcontrib>ROMANOVA ANNA NIKOLAEVNA</creatorcontrib><creatorcontrib>NIKITINA IRINA VALENTINOVNA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GUSAKOV ALEKSANDR VASIL'EVICH</au><au>NADTOCHEEVA VALENTINA MAKSIMOVNA</au><au>ROMANOVA ANNA NIKOLAEVNA</au><au>NIKITINA IRINA VALENTINOVNA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCTION OF SYNTHETIC TECHNICAL CLOTH EDGE</title><date>2009-10-27</date><risdate>2009</risdate><abstract>FIELD: technological processes. ^ SUBSTANCE: edge of cloth consists of reinforced structure adjacent to solder and made of web threads and polypropylene binder. Web is thermally shrunk, cut along its width by a cutting tool with a temperature of 450-650C to make a solder and introduction of polymer binder melt from upper and lower sides of web. Melt is supplied under pressure from extruder. As polymer binder they use polypropylene with index of melt fluidity of 0.6-15. Amount of polymer applied per unit of web length is defined depending on thickness of web, surface density, width of edge, total number of main and weft thread types, from which the web is woven, density of material thread, weight portion of thread in web, volume shrinkage of melt and density of polypropylene. ^ EFFECT: improved mechanical and hydrolytic stability at high temperatures in atmosphere of high humidity, and resistance to side impact and abrasive loads. ^ 3 cl, 1 dwg, 3 tbl Изобретение относится к способу получения кромок синтетических технических полотен, в частности сушильных сеток бумаго- и картоноделательных машин. Кромка полотна состоит из примыкающей к припаю армированной структуры из нитей сетки и полипропиленового связующего. Осуществляют термоусадку сетки, обрезание ее по ширине режущим инструментом с температурой 450-650°С с образованием припая и внесение с верхней и нижней сторон сетки расплава полимерного связующего. Расплав поступает под давлением из экструдера. В качестве полимерного связующего используют полипропилен с индексом текучести расплава 0,6-15. Количество наносимого на единицу длины полотна полимера определяют в зависимости от толщины сетки, поверхностной плотности, ширины кромки, общего числа видов основных и уточных нитей, из которых соткана сетка, плотности материала нити, массовой доли нити в сетке, объемной усадки расплава и плотности полипропилена. Кромка, полученная данным способом, обладает увеличенной механической и гидролитической устойчивостью при температурах выше 100°С в атмосфере высокой влажности, а также сопротивлением к боковым ударным и абразивным нагрузкам. 2 з.п. ф-лы, 1 ил., 3 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2371534C1
source esp@cenet
subjects METHODS OF PRODUCING PAPER THEREON
PAPER-MAKING
PAPER-MAKING MACHINES
PRODUCTION OF CELLULOSE
TEXTILES
title METHOD FOR PRODUCTION OF SYNTHETIC TECHNICAL CLOTH EDGE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-14T14%3A27%3A12IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GUSAKOV%20ALEKSANDR%20VASIL'EVICH&rft.date=2009-10-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2371534C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true