METHOD FOR PREPARATION OF ACTIVE CHARCOAL

FIELD: chemistry. ^ SUBSTANCE: method for active charcoal preparation includes aspen wood pyrolysis, desintegration of the obtained charcoal up to particle size 0.2-2.0 mm, activation with hydrogen peroxide at temperature 250-300C and pressure 30-50 MPa during 5-10 min, separation, washing with dist...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: PATJAKIN VASILIJ IVANOVICH, PIL'SHCHIKOV JURIJ NIKOLAEVICH, SPITSYN ANDREJ ALEKSANDROVICH, BIRMAN ALEKSEJ ROMANOVICH, TEPPOEV ALEKSEJ VIKTOROVICH, BELONOGOVA NATAL'JA ALEKSANDROVNA
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: chemistry. ^ SUBSTANCE: method for active charcoal preparation includes aspen wood pyrolysis, desintegration of the obtained charcoal up to particle size 0.2-2.0 mm, activation with hydrogen peroxide at temperature 250-300C and pressure 30-50 MPa during 5-10 min, separation, washing with distilled water and drying. ^ EFFECT: obtaining of quality charcoal able to effective sorption of the benzene from water media. ^ 2 tbl Изобретение относится к сорбционной технике и может быть использовано для производства адсорбента - активированного древесного угля. Способ получения активированного древесного угля включает пиролиз древесины осины, измельчение полученного древесного угля до размера частиц 0,2-2,0 мм, активацию пероксидом водорода при температуре 250-300°C в течение 5-10 минут при давлении 30-50 МПа, сепарацию, промывку дистиллированной водой и сушку. Изобретение позволяет получить качественный уголь, способный к эффективной сорбции бензола из водных сред. 2 табл.