GROUTING MORTAR "á Ñÿ£òÜ-Æ£"
FIELD: construction. ^ SUBSTANCE: grouting mortar contains, wt %: hydraulic binding agent - 70-85, surface active agent - SAA "Éæá" - 0.1-0.2, SAA "äé ÆÜ-" - 0.1-0.3, hydrocarbon phase is the rest of the mortar. Construction gypsum is used hydraulic binding agent at grouting mort...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: construction. ^ SUBSTANCE: grouting mortar contains, wt %: hydraulic binding agent - 70-85, surface active agent - SAA "Éæá" - 0.1-0.2, SAA "äé ÆÜ-" - 0.1-0.3, hydrocarbon phase is the rest of the mortar. Construction gypsum is used hydraulic binding agent at grouting mortar density to 1.45 g/cm3. ^ EFFECT: improved flow characteristics, sedimentation stability and resistance to corrosive medium, preservation of grout properties. ^ 2 cl, 1 tbl, 1 ex
Изобретение относится к строительству скважин различного назначения и, в частности, к ремонтно-изоляционным работам в скважинах и/или при ликвидации водопроявлений в процессе бурения скважин. Тампонажный раствор содержит, мас.%: гидравлическое вяжущее - 70-85, поверхностно-активное вещество - ПАВ «АБР» - 0,1-0,2, ПАВ «нефтенол ВКС-Н» - 0,1-0,3, углеводородная фаза - остальное. При плотности тампонажного раствора до 1,45 г/см3 в качестве гидравлического вяжущего применен строительный гипс. Технический результат - повышение реологических свойств, стабильности, седиментационной устойчивости от 1 до 10 сут, стойкости в агрессивных средах, сохранение свойств раствора в интервале температур от 20 до +200°С. 1 з.п. ф-лы, 1 табл. |
---|