METHOD OF COMPOSITION COATING RECEIVING

FIELD: metallurgy. ^ SUBSTANCE: method includes preparation of aqueous suspension of detonating nanodiamonds, introduction of aqueous suspension into electrolyte for coatings sedimentation and electrolysis, herewith aqueous suspension, consisting 1-5 % of detonating nanodiamonds, for disaggregation...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LARIONOVA IRINA SEMENOVNA, BELJAEV VJACHESLAV NIKOLAEVICH, IL'INYKH KONSTANTIN FEDOROVICH, MITROFANOV VJACHESLAV MIKHAJLOVICH, FROLOV ALEKSANDR VALERIEVICH, BYCHIN NIKOLAJ VALER'EVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LARIONOVA IRINA SEMENOVNA
BELJAEV VJACHESLAV NIKOLAEVICH
IL'INYKH KONSTANTIN FEDOROVICH
MITROFANOV VJACHESLAV MIKHAJLOVICH
FROLOV ALEKSANDR VALERIEVICH
BYCHIN NIKOLAJ VALER'EVICH
description FIELD: metallurgy. ^ SUBSTANCE: method includes preparation of aqueous suspension of detonating nanodiamonds, introduction of aqueous suspension into electrolyte for coatings sedimentation and electrolysis, herewith aqueous suspension, consisting 1-5 % of detonating nanodiamonds, for disaggregation is subject to treatment on rotary-pulsating or ultrasonic device or on disintegrator, is heated during 2 hours in 15 % boric acid solution with sediment washing from acid surplus up to meanings pH 3.5-6.0, then is treated during 2 hours by 0.5-2.0 % sodium alkali solution with following removing of alkali surplus up to meanings pH 6.0-8.0. ^ EFFECT: increasing of process manufacturability, expansion of operational functionality and efficiency of nanosized discontinuous phase, elimination of resource- and power-intensive external action on electrolyte during the process of coating receivin. ^ 2 tbl, 3 dwg, 2 ex Изобретение относится к области гальванотехники. Способ включает приготовление водной суспензии детонационных наноалмазов, введение водной суспензии в электролит для осаждения покрытия и электролиз, при этом водную суспензию, содержащую 1-5% детонационных наноалмазов, для дезагрегации подвергают обработке на роторно-пульсационной или ультразвуковой установке или на дезинтеграторе, нагревают 2 часа в 15% растворе соляной кислоты с отмывкой осадка от избытка кислоты до значений рН 3,5-6,0, затем обрабатывают 2 часа 0,5-2,0% раствором натриевой щелочи с последующим удалением избытка щелочи до значений рН 6,0-8,0. Технический результат: повышение технологичности процесса, расширение эксплуатационных возможностей и эффективности использования наноразмерной дисперсной фазы, исключение ресурсо- и энергоемких внешних воздействий на электролит в процессе получения покрытия. 2 табл., 3 ил.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2357017C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2357017C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2357017C13</originalsourceid><addsrcrecordid>eNrjZFD3dQ3x8HdR8HdTcPb3DfAP9gzx9PcDsh1DPP3cFYJcnV09w4AsHgbWtMSc4lReKM3NoODmGuLsoZtakB-fWlyQmJyal1oSHxRqZGxqbmBo7mxoTIQSAKjMI5s</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF COMPOSITION COATING RECEIVING</title><source>esp@cenet</source><creator>LARIONOVA IRINA SEMENOVNA ; BELJAEV VJACHESLAV NIKOLAEVICH ; IL'INYKH KONSTANTIN FEDOROVICH ; MITROFANOV VJACHESLAV MIKHAJLOVICH ; FROLOV ALEKSANDR VALERIEVICH ; BYCHIN NIKOLAJ VALER'EVICH</creator><creatorcontrib>LARIONOVA IRINA SEMENOVNA ; BELJAEV VJACHESLAV NIKOLAEVICH ; IL'INYKH KONSTANTIN FEDOROVICH ; MITROFANOV VJACHESLAV MIKHAJLOVICH ; FROLOV ALEKSANDR VALERIEVICH ; BYCHIN NIKOLAJ VALER'EVICH</creatorcontrib><description>FIELD: metallurgy. ^ SUBSTANCE: method includes preparation of aqueous suspension of detonating nanodiamonds, introduction of aqueous suspension into electrolyte for coatings sedimentation and electrolysis, herewith aqueous suspension, consisting 1-5 % of detonating nanodiamonds, for disaggregation is subject to treatment on rotary-pulsating or ultrasonic device or on disintegrator, is heated during 2 hours in 15 % boric acid solution with sediment washing from acid surplus up to meanings pH 3.5-6.0, then is treated during 2 hours by 0.5-2.0 % sodium alkali solution with following removing of alkali surplus up to meanings pH 6.0-8.0. ^ EFFECT: increasing of process manufacturability, expansion of operational functionality and efficiency of nanosized discontinuous phase, elimination of resource- and power-intensive external action on electrolyte during the process of coating receivin. ^ 2 tbl, 3 dwg, 2 ex Изобретение относится к области гальванотехники. Способ включает приготовление водной суспензии детонационных наноалмазов, введение водной суспензии в электролит для осаждения покрытия и электролиз, при этом водную суспензию, содержащую 1-5% детонационных наноалмазов, для дезагрегации подвергают обработке на роторно-пульсационной или ультразвуковой установке или на дезинтеграторе, нагревают 2 часа в 15% растворе соляной кислоты с отмывкой осадка от избытка кислоты до значений рН 3,5-6,0, затем обрабатывают 2 часа 0,5-2,0% раствором натриевой щелочи с последующим удалением избытка щелочи до значений рН 6,0-8,0. Технический результат: повышение технологичности процесса, расширение эксплуатационных возможностей и эффективности использования наноразмерной дисперсной фазы, исключение ресурсо- и энергоемких внешних воздействий на электролит в процессе получения покрытия. 2 табл., 3 ил.</description><language>eng ; rus</language><subject>APPARATUS THEREFOR ; CHEMISTRY ; ELECTROFORMING ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; METALLURGY ; PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090527&amp;DB=EPODOC&amp;CC=RU&amp;NR=2357017C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090527&amp;DB=EPODOC&amp;CC=RU&amp;NR=2357017C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LARIONOVA IRINA SEMENOVNA</creatorcontrib><creatorcontrib>BELJAEV VJACHESLAV NIKOLAEVICH</creatorcontrib><creatorcontrib>IL'INYKH KONSTANTIN FEDOROVICH</creatorcontrib><creatorcontrib>MITROFANOV VJACHESLAV MIKHAJLOVICH</creatorcontrib><creatorcontrib>FROLOV ALEKSANDR VALERIEVICH</creatorcontrib><creatorcontrib>BYCHIN NIKOLAJ VALER'EVICH</creatorcontrib><title>METHOD OF COMPOSITION COATING RECEIVING</title><description>FIELD: metallurgy. ^ SUBSTANCE: method includes preparation of aqueous suspension of detonating nanodiamonds, introduction of aqueous suspension into electrolyte for coatings sedimentation and electrolysis, herewith aqueous suspension, consisting 1-5 % of detonating nanodiamonds, for disaggregation is subject to treatment on rotary-pulsating or ultrasonic device or on disintegrator, is heated during 2 hours in 15 % boric acid solution with sediment washing from acid surplus up to meanings pH 3.5-6.0, then is treated during 2 hours by 0.5-2.0 % sodium alkali solution with following removing of alkali surplus up to meanings pH 6.0-8.0. ^ EFFECT: increasing of process manufacturability, expansion of operational functionality and efficiency of nanosized discontinuous phase, elimination of resource- and power-intensive external action on electrolyte during the process of coating receivin. ^ 2 tbl, 3 dwg, 2 ex Изобретение относится к области гальванотехники. Способ включает приготовление водной суспензии детонационных наноалмазов, введение водной суспензии в электролит для осаждения покрытия и электролиз, при этом водную суспензию, содержащую 1-5% детонационных наноалмазов, для дезагрегации подвергают обработке на роторно-пульсационной или ультразвуковой установке или на дезинтеграторе, нагревают 2 часа в 15% растворе соляной кислоты с отмывкой осадка от избытка кислоты до значений рН 3,5-6,0, затем обрабатывают 2 часа 0,5-2,0% раствором натриевой щелочи с последующим удалением избытка щелочи до значений рН 6,0-8,0. Технический результат: повышение технологичности процесса, расширение эксплуатационных возможностей и эффективности использования наноразмерной дисперсной фазы, исключение ресурсо- и энергоемких внешних воздействий на электролит в процессе получения покрытия. 2 табл., 3 ил.</description><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>ELECTROFORMING</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>METALLURGY</subject><subject>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD3dQ3x8HdR8HdTcPb3DfAP9gzx9PcDsh1DPP3cFYJcnV09w4AsHgbWtMSc4lReKM3NoODmGuLsoZtakB-fWlyQmJyal1oSHxRqZGxqbmBo7mxoTIQSAKjMI5s</recordid><startdate>20090527</startdate><enddate>20090527</enddate><creator>LARIONOVA IRINA SEMENOVNA</creator><creator>BELJAEV VJACHESLAV NIKOLAEVICH</creator><creator>IL'INYKH KONSTANTIN FEDOROVICH</creator><creator>MITROFANOV VJACHESLAV MIKHAJLOVICH</creator><creator>FROLOV ALEKSANDR VALERIEVICH</creator><creator>BYCHIN NIKOLAJ VALER'EVICH</creator><scope>EVB</scope></search><sort><creationdate>20090527</creationdate><title>METHOD OF COMPOSITION COATING RECEIVING</title><author>LARIONOVA IRINA SEMENOVNA ; BELJAEV VJACHESLAV NIKOLAEVICH ; IL'INYKH KONSTANTIN FEDOROVICH ; MITROFANOV VJACHESLAV MIKHAJLOVICH ; FROLOV ALEKSANDR VALERIEVICH ; BYCHIN NIKOLAJ VALER'EVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2357017C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2009</creationdate><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>ELECTROFORMING</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>METALLURGY</topic><topic>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</topic><toplevel>online_resources</toplevel><creatorcontrib>LARIONOVA IRINA SEMENOVNA</creatorcontrib><creatorcontrib>BELJAEV VJACHESLAV NIKOLAEVICH</creatorcontrib><creatorcontrib>IL'INYKH KONSTANTIN FEDOROVICH</creatorcontrib><creatorcontrib>MITROFANOV VJACHESLAV MIKHAJLOVICH</creatorcontrib><creatorcontrib>FROLOV ALEKSANDR VALERIEVICH</creatorcontrib><creatorcontrib>BYCHIN NIKOLAJ VALER'EVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LARIONOVA IRINA SEMENOVNA</au><au>BELJAEV VJACHESLAV NIKOLAEVICH</au><au>IL'INYKH KONSTANTIN FEDOROVICH</au><au>MITROFANOV VJACHESLAV MIKHAJLOVICH</au><au>FROLOV ALEKSANDR VALERIEVICH</au><au>BYCHIN NIKOLAJ VALER'EVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF COMPOSITION COATING RECEIVING</title><date>2009-05-27</date><risdate>2009</risdate><abstract>FIELD: metallurgy. ^ SUBSTANCE: method includes preparation of aqueous suspension of detonating nanodiamonds, introduction of aqueous suspension into electrolyte for coatings sedimentation and electrolysis, herewith aqueous suspension, consisting 1-5 % of detonating nanodiamonds, for disaggregation is subject to treatment on rotary-pulsating or ultrasonic device or on disintegrator, is heated during 2 hours in 15 % boric acid solution with sediment washing from acid surplus up to meanings pH 3.5-6.0, then is treated during 2 hours by 0.5-2.0 % sodium alkali solution with following removing of alkali surplus up to meanings pH 6.0-8.0. ^ EFFECT: increasing of process manufacturability, expansion of operational functionality and efficiency of nanosized discontinuous phase, elimination of resource- and power-intensive external action on electrolyte during the process of coating receivin. ^ 2 tbl, 3 dwg, 2 ex Изобретение относится к области гальванотехники. Способ включает приготовление водной суспензии детонационных наноалмазов, введение водной суспензии в электролит для осаждения покрытия и электролиз, при этом водную суспензию, содержащую 1-5% детонационных наноалмазов, для дезагрегации подвергают обработке на роторно-пульсационной или ультразвуковой установке или на дезинтеграторе, нагревают 2 часа в 15% растворе соляной кислоты с отмывкой осадка от избытка кислоты до значений рН 3,5-6,0, затем обрабатывают 2 часа 0,5-2,0% раствором натриевой щелочи с последующим удалением избытка щелочи до значений рН 6,0-8,0. Технический результат: повышение технологичности процесса, расширение эксплуатационных возможностей и эффективности использования наноразмерной дисперсной фазы, исключение ресурсо- и энергоемких внешних воздействий на электролит в процессе получения покрытия. 2 табл., 3 ил.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2357017C1
source esp@cenet
subjects APPARATUS THEREFOR
CHEMISTRY
ELECTROFORMING
ELECTROLYTIC OR ELECTROPHORETIC PROCESSES
METALLURGY
PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS
title METHOD OF COMPOSITION COATING RECEIVING
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-13T11%3A15%3A31IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LARIONOVA%20IRINA%20SEMENOVNA&rft.date=2009-05-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2357017C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true