AMORPHOUS RESISTIVE ALLOY ON BASIS OF NICKEL

FIELD: metallurgy. ^ SUBSTANCE: invention relates to precision alloys metallurgy, which are used for microwire casting in glass insulation. Amorphous resistive alloy on the basis of nickel contains components in a following ratio (wt %): chromium 6.0 - 14.0, silicon 4.0 - 6.0, boron 1.3 - 2.0, galli...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SOMKOVA EKATERINA ALEKSANDROVNA, TOCHENJUK DAR'JA ALEKSANDROVNA, FARMAKOVSKIJ BORIS VLADIMIROVICH, JURKOV MAKSIM ANATOL'EVICH, SEMENOV ALEKSANDR SERGEEVICH, BYSTROV RUSLAN JUR'EVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SOMKOVA EKATERINA ALEKSANDROVNA
TOCHENJUK DAR'JA ALEKSANDROVNA
FARMAKOVSKIJ BORIS VLADIMIROVICH
JURKOV MAKSIM ANATOL'EVICH
SEMENOV ALEKSANDR SERGEEVICH
BYSTROV RUSLAN JUR'EVICH
description FIELD: metallurgy. ^ SUBSTANCE: invention relates to precision alloys metallurgy, which are used for microwire casting in glass insulation. Amorphous resistive alloy on the basis of nickel contains components in a following ratio (wt %): chromium 6.0 - 14.0, silicon 4.0 - 6.0, boron 1.3 - 2.0, gallium 4.0 - 6.0, zirconium 6.0 - 8.0, yttrium 0.2 - 0.6, cerium 0.05 - 0.2, lanthanum 0.05 -0.2, nickel - the rest. Invention is directed to receiving of amorphous structure of resistive alloy, increasing of cold resistance till - 196C and strength-to-weigth ratio at those temperatures. ^ EFFECT: receiving of alloy on the basis of nickel, which keep low temperature coefficient of resistance, high temperature-timing stability and well wettability with glasses of borosilicate group in conditions of microwire casting. ^ 1 tbl, 1 dwg Изобретение относится к металлургии прецизионных сплавов, которые применимы для литья микропроводов в стеклянной изоляции. Аморфный резистивный сплав на основе никеля содержит компоненты в следующем соотношении, мас.%: хром 6,0-14,0, кремний 4,0-6,0, бор 1,3-2,0, галлий 4,0-6,0, цирконий 6,0-8,0, иттрий 0,2-0,6, церий 0,05-0,2, лантан 0,05-0,2, никель - остальное. Изобретение направлено на получение аморфной структуры резистивного сплава, повышение хладостойкости до -196°С и удельной прочности при этих температурах. При этом аморфный резистивный сплав сохраняет низкий температурный коэффициент сопротивления, высокую температурно-временную стабильность и хорошую смачиваемость со стеклами боросиликатной группы в условиях литья микропроводов. 1 ил., 1 табл.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2351672C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2351672C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2351672C23</originalsourceid><addsrcrecordid>eNrjZNBx9PUPCvDwDw1WCHIN9gwO8QxzVXD08fGPVPD3U3ByBAop-Lsp-Hk6e7v68DCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQI2NTQzNzI2cjYyKUAABcaCTw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>AMORPHOUS RESISTIVE ALLOY ON BASIS OF NICKEL</title><source>esp@cenet</source><creator>SOMKOVA EKATERINA ALEKSANDROVNA ; TOCHENJUK DAR'JA ALEKSANDROVNA ; FARMAKOVSKIJ BORIS VLADIMIROVICH ; JURKOV MAKSIM ANATOL'EVICH ; SEMENOV ALEKSANDR SERGEEVICH ; BYSTROV RUSLAN JUR'EVICH</creator><creatorcontrib>SOMKOVA EKATERINA ALEKSANDROVNA ; TOCHENJUK DAR'JA ALEKSANDROVNA ; FARMAKOVSKIJ BORIS VLADIMIROVICH ; JURKOV MAKSIM ANATOL'EVICH ; SEMENOV ALEKSANDR SERGEEVICH ; BYSTROV RUSLAN JUR'EVICH</creatorcontrib><description>FIELD: metallurgy. ^ SUBSTANCE: invention relates to precision alloys metallurgy, which are used for microwire casting in glass insulation. Amorphous resistive alloy on the basis of nickel contains components in a following ratio (wt %): chromium 6.0 - 14.0, silicon 4.0 - 6.0, boron 1.3 - 2.0, gallium 4.0 - 6.0, zirconium 6.0 - 8.0, yttrium 0.2 - 0.6, cerium 0.05 - 0.2, lanthanum 0.05 -0.2, nickel - the rest. Invention is directed to receiving of amorphous structure of resistive alloy, increasing of cold resistance till - 196C and strength-to-weigth ratio at those temperatures. ^ EFFECT: receiving of alloy on the basis of nickel, which keep low temperature coefficient of resistance, high temperature-timing stability and well wettability with glasses of borosilicate group in conditions of microwire casting. ^ 1 tbl, 1 dwg Изобретение относится к металлургии прецизионных сплавов, которые применимы для литья микропроводов в стеклянной изоляции. Аморфный резистивный сплав на основе никеля содержит компоненты в следующем соотношении, мас.%: хром 6,0-14,0, кремний 4,0-6,0, бор 1,3-2,0, галлий 4,0-6,0, цирконий 6,0-8,0, иттрий 0,2-0,6, церий 0,05-0,2, лантан 0,05-0,2, никель - остальное. Изобретение направлено на получение аморфной структуры резистивного сплава, повышение хладостойкости до -196°С и удельной прочности при этих температурах. При этом аморфный резистивный сплав сохраняет низкий температурный коэффициент сопротивления, высокую температурно-временную стабильность и хорошую смачиваемость со стеклами боросиликатной группы в условиях литья микропроводов. 1 ил., 1 табл.</description><language>eng ; rus</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090410&amp;DB=EPODOC&amp;CC=RU&amp;NR=2351672C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090410&amp;DB=EPODOC&amp;CC=RU&amp;NR=2351672C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SOMKOVA EKATERINA ALEKSANDROVNA</creatorcontrib><creatorcontrib>TOCHENJUK DAR'JA ALEKSANDROVNA</creatorcontrib><creatorcontrib>FARMAKOVSKIJ BORIS VLADIMIROVICH</creatorcontrib><creatorcontrib>JURKOV MAKSIM ANATOL'EVICH</creatorcontrib><creatorcontrib>SEMENOV ALEKSANDR SERGEEVICH</creatorcontrib><creatorcontrib>BYSTROV RUSLAN JUR'EVICH</creatorcontrib><title>AMORPHOUS RESISTIVE ALLOY ON BASIS OF NICKEL</title><description>FIELD: metallurgy. ^ SUBSTANCE: invention relates to precision alloys metallurgy, which are used for microwire casting in glass insulation. Amorphous resistive alloy on the basis of nickel contains components in a following ratio (wt %): chromium 6.0 - 14.0, silicon 4.0 - 6.0, boron 1.3 - 2.0, gallium 4.0 - 6.0, zirconium 6.0 - 8.0, yttrium 0.2 - 0.6, cerium 0.05 - 0.2, lanthanum 0.05 -0.2, nickel - the rest. Invention is directed to receiving of amorphous structure of resistive alloy, increasing of cold resistance till - 196C and strength-to-weigth ratio at those temperatures. ^ EFFECT: receiving of alloy on the basis of nickel, which keep low temperature coefficient of resistance, high temperature-timing stability and well wettability with glasses of borosilicate group in conditions of microwire casting. ^ 1 tbl, 1 dwg Изобретение относится к металлургии прецизионных сплавов, которые применимы для литья микропроводов в стеклянной изоляции. Аморфный резистивный сплав на основе никеля содержит компоненты в следующем соотношении, мас.%: хром 6,0-14,0, кремний 4,0-6,0, бор 1,3-2,0, галлий 4,0-6,0, цирконий 6,0-8,0, иттрий 0,2-0,6, церий 0,05-0,2, лантан 0,05-0,2, никель - остальное. Изобретение направлено на получение аморфной структуры резистивного сплава, повышение хладостойкости до -196°С и удельной прочности при этих температурах. При этом аморфный резистивный сплав сохраняет низкий температурный коэффициент сопротивления, высокую температурно-временную стабильность и хорошую смачиваемость со стеклами боросиликатной группы в условиях литья микропроводов. 1 ил., 1 табл.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNBx9PUPCvDwDw1WCHIN9gwO8QxzVXD08fGPVPD3U3ByBAop-Lsp-Hk6e7v68DCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQI2NTQzNzI2cjYyKUAABcaCTw</recordid><startdate>20090410</startdate><enddate>20090410</enddate><creator>SOMKOVA EKATERINA ALEKSANDROVNA</creator><creator>TOCHENJUK DAR'JA ALEKSANDROVNA</creator><creator>FARMAKOVSKIJ BORIS VLADIMIROVICH</creator><creator>JURKOV MAKSIM ANATOL'EVICH</creator><creator>SEMENOV ALEKSANDR SERGEEVICH</creator><creator>BYSTROV RUSLAN JUR'EVICH</creator><scope>EVB</scope></search><sort><creationdate>20090410</creationdate><title>AMORPHOUS RESISTIVE ALLOY ON BASIS OF NICKEL</title><author>SOMKOVA EKATERINA ALEKSANDROVNA ; TOCHENJUK DAR'JA ALEKSANDROVNA ; FARMAKOVSKIJ BORIS VLADIMIROVICH ; JURKOV MAKSIM ANATOL'EVICH ; SEMENOV ALEKSANDR SERGEEVICH ; BYSTROV RUSLAN JUR'EVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2351672C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2009</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>SOMKOVA EKATERINA ALEKSANDROVNA</creatorcontrib><creatorcontrib>TOCHENJUK DAR'JA ALEKSANDROVNA</creatorcontrib><creatorcontrib>FARMAKOVSKIJ BORIS VLADIMIROVICH</creatorcontrib><creatorcontrib>JURKOV MAKSIM ANATOL'EVICH</creatorcontrib><creatorcontrib>SEMENOV ALEKSANDR SERGEEVICH</creatorcontrib><creatorcontrib>BYSTROV RUSLAN JUR'EVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SOMKOVA EKATERINA ALEKSANDROVNA</au><au>TOCHENJUK DAR'JA ALEKSANDROVNA</au><au>FARMAKOVSKIJ BORIS VLADIMIROVICH</au><au>JURKOV MAKSIM ANATOL'EVICH</au><au>SEMENOV ALEKSANDR SERGEEVICH</au><au>BYSTROV RUSLAN JUR'EVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>AMORPHOUS RESISTIVE ALLOY ON BASIS OF NICKEL</title><date>2009-04-10</date><risdate>2009</risdate><abstract>FIELD: metallurgy. ^ SUBSTANCE: invention relates to precision alloys metallurgy, which are used for microwire casting in glass insulation. Amorphous resistive alloy on the basis of nickel contains components in a following ratio (wt %): chromium 6.0 - 14.0, silicon 4.0 - 6.0, boron 1.3 - 2.0, gallium 4.0 - 6.0, zirconium 6.0 - 8.0, yttrium 0.2 - 0.6, cerium 0.05 - 0.2, lanthanum 0.05 -0.2, nickel - the rest. Invention is directed to receiving of amorphous structure of resistive alloy, increasing of cold resistance till - 196C and strength-to-weigth ratio at those temperatures. ^ EFFECT: receiving of alloy on the basis of nickel, which keep low temperature coefficient of resistance, high temperature-timing stability and well wettability with glasses of borosilicate group in conditions of microwire casting. ^ 1 tbl, 1 dwg Изобретение относится к металлургии прецизионных сплавов, которые применимы для литья микропроводов в стеклянной изоляции. Аморфный резистивный сплав на основе никеля содержит компоненты в следующем соотношении, мас.%: хром 6,0-14,0, кремний 4,0-6,0, бор 1,3-2,0, галлий 4,0-6,0, цирконий 6,0-8,0, иттрий 0,2-0,6, церий 0,05-0,2, лантан 0,05-0,2, никель - остальное. Изобретение направлено на получение аморфной структуры резистивного сплава, повышение хладостойкости до -196°С и удельной прочности при этих температурах. При этом аморфный резистивный сплав сохраняет низкий температурный коэффициент сопротивления, высокую температурно-временную стабильность и хорошую смачиваемость со стеклами боросиликатной группы в условиях литья микропроводов. 1 ил., 1 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2351672C2
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title AMORPHOUS RESISTIVE ALLOY ON BASIS OF NICKEL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T10%3A10%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SOMKOVA%20EKATERINA%20ALEKSANDROVNA&rft.date=2009-04-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2351672C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true