METHOD OF OBTAINING FINE CRYSTALLINE CORUNDUM

FIELD: chemistry. ^ SUBSTANCE: method includes processing of aluminium hydroxide or of aluminuim oxyhydroxide in presence of water vapour with temperature changing from 20 to 400-450C with rate 2-150/hour with further stand at reached temperature during 10-72 hours. Water vapour pressure at temperat...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: IVAKIN JURIJ DMITRIEVICH, PANASJUK GEORGIJ PAVLOVICH, TORBIN SERGEJ NIKOLAEVICH, DANCHEVSKAJA MARINA NIKOLAEVNA
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: chemistry. ^ SUBSTANCE: method includes processing of aluminium hydroxide or of aluminuim oxyhydroxide in presence of water vapour with temperature changing from 20 to 400-450C with rate 2-150/hour with further stand at reached temperature during 10-72 hours. Water vapour pressure at temperature 400-450C is selected in interval 3-40 MPa. ^ EFFECT: obtaining fine crystalline corundum. ^ 4 ex