METHOD OF PRODUCING POOR POROUS POWDER MATERIALS

FIELD: metallurgy; technological processes. ^ SUBSTANCE: shavings of low-melt material are filled into die-mold at amount of 26-48 wt % and preliminary pressing is performed at pressure of 600-620 MPa. Then iron powder is filled and a final pressing is carried out at 260-620 MPa producing two-layer...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SERGEENKO SERGEJ NIKOLAEVICH, DOROFEEV JURIJ GRIGOR'EVICH, ROMACHEVSKIJ EVGENIJ VASIL'EVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: metallurgy; technological processes. ^ SUBSTANCE: shavings of low-melt material are filled into die-mold at amount of 26-48 wt % and preliminary pressing is performed at pressure of 600-620 MPa. Then iron powder is filled and a final pressing is carried out at 260-620 MPa producing two-layer blank. The produced blank is sintered in a glass melt and simultaneously impregnated with a low-melt material. ^ EFFECT: method facilitates increasing amount of utilised shavings and decreasing prime cost of produced materials. ^ 1 dwg, 3 ex