METHOD OF MANUFACTURE OF INTERMEDIATE BLANK FROM alpha- OR alpha+beta-TITANIUM ALLOYS

FIELD: manufacture of intermediate blanks from alpha- and alpha+beta-titanium alloys by hot deformation method. ^ SUBSTANCE: proposed method includes forging an ingot into bar during several passes at temperature of beta- and (alpha+beta) field. Then, blank is subjected to machining and two-stage he...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LEVIN IGOR' VASIL'EVICH, SMIRNOV VLADIMIR GRIGOR'EVICH, TETJUKHIN VLADISLAV VALENTINOVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: manufacture of intermediate blanks from alpha- and alpha+beta-titanium alloys by hot deformation method. ^ SUBSTANCE: proposed method includes forging an ingot into bar during several passes at temperature of beta- and (alpha+beta) field. Then, blank is subjected to machining and two-stage heating. At the first stage, blank is heated to temperature of its surface which is below polymorphous transformation temperature by 250 C and is above polymorphous transformation temperature by 100 C; heating is performed at rate of 0.3-2.5°C/s. At the second stage, blank is cooled down or heated to temperature which is below polymorphous transformation temperature by 40-250 C. Final molding is performed in (alpha+beta) field at forging reduction ratio at last passes of 1.36-2.5. ^ EFFECT: reduction of blank heating time to molding temperature; increased productivity; possibility of obtaining fine-grain structure of blank metal. ^ 2 cl, 3 ex