METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-BORON ALLOY-BASED COAT
FIELD: electrolytic deposition of hard, wear resistant coats, in particular iron-boron coats useful in surface reducing and hardening. ^ SUBSTANCE: claimed method includes coat deposition from electrolyte containing (kg/m3): boric acid 2.5-60; iron (II) chloride 300-450; hydrochloric acid 0.5-1.5 an...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: electrolytic deposition of hard, wear resistant coats, in particular iron-boron coats useful in surface reducing and hardening. ^ SUBSTANCE: claimed method includes coat deposition from electrolyte containing (kg/m3): boric acid 2.5-60; iron (II) chloride 300-450; hydrochloric acid 0.5-1.5 and water, by using alternate asymmetric current with asymmetric coefficient of 1.2-6; cathode current density of 15-60 A/dm3, at electrolyte temperature of 20-40°C and pH 0.8. Method of present invention makes it possible to increase capability and deposition rate; to decrease electrolyte temperature; and to improve cohesive resistance between coat and support. ^ EFFECT: coats of increased microhardness and wear resistance. ^ 1 ex |
---|