MAMMARY GLAND EXOPROSTHESIS

medical engineering. SUBSTANCE: device is manufactured from polyvinyl chloride plastizole, dioctyl pthalate and polyethylsiloxane fluid taken in 30-50:60-30:10-20 mass proportion, respectively. Cross-linking temperature is from 25-30 C to 210-215 C, heat time is 30-40 min at 210-215 C with gradual t...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: MAKHORTOV N.S
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:medical engineering. SUBSTANCE: device is manufactured from polyvinyl chloride plastizole, dioctyl pthalate and polyethylsiloxane fluid taken in 30-50:60-30:10-20 mass proportion, respectively. Cross-linking temperature is from 25-30 C to 210-215 C, heat time is 30-40 min at 210-215 C with gradual temperature reduction to 25-30 C during 50-60 min. EFFECT: enhanced reliability and strength. 1 tbl