METHOD OF PREPARING SILICON OXIDE SYSTEMS

fiber optics. SUBSTANCE: 35% polysilicic acid sol is poured into apparatus and frozen by liquid nitrogen, liquid oxygen, liquid ammonia, or liquid inert gases. Intake and temperature of cooling agent are maintained such as to provide value of specific heat current through sol-ice interface equal to...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TUROVEROV P.K, KUZNETSOVA R.V, ERMOLENKO T.A, KUZNETSOV A.I, EVLAMPIEV I.K, RASTORGUEV JU.I, OLEJNIKOVA B.I, ELISEEV N.P, CHEREMISIN I.I, POPOV S.A
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:fiber optics. SUBSTANCE: 35% polysilicic acid sol is poured into apparatus and frozen by liquid nitrogen, liquid oxygen, liquid ammonia, or liquid inert gases. Intake and temperature of cooling agent are maintained such as to provide value of specific heat current through sol-ice interface equal to (0.8-15) x 103 J/sq.m s. One hour after freezing, heating is turned on and formed gel is unfrozen. Solid and liquid phases are separated. Silicon dioxide thus obtained is dried and thermally treated to give product with specified granulometric composition with deviation from major fraction no more than by 20%. Product can be used for manufacture of quartz optic fiber. EFFECT: optimized preparation parameters. 1 tbl