METHOD FOR REDUCING OPEN-CIRCUIT VOLTAGE OF CHEMICAL CURRENT SUPPLY
chemical lithium current supplies. SUBSTANCE: method for reducing open-circuit voltage of Li- CuO current supply to 1.8-2.0 V by partial discharge without decreasing its capacity involves potential static discharge of newly manufactured chemical current supply at a voltage of 1.5-1.6 V for 1-2 h unt...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | chemical lithium current supplies. SUBSTANCE: method for reducing open-circuit voltage of Li- CuO current supply to 1.8-2.0 V by partial discharge without decreasing its capacity involves potential static discharge of newly manufactured chemical current supply at a voltage of 1.5-1.6 V for 1-2 h until stabilized current is obtained. EFFECT: facilitated procedure. 1 tbl |
---|