FLUIDIZED BED PROCESS FOR BORON-NICKELIZING OF STEEL OBJECTS
FIELD: metal coatings. SUBSTANCE: process involves preliminarily saturation of nickel at 350-500 C during 5 to 30 min and saturation with boron at 600 to 950 C. The former is conducted in composition containing, wt %: nickel oxide 0.02-0.5, boron carbide 5-35, ammonium chloride 0.005-0.2, sodium tet...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: metal coatings. SUBSTANCE: process involves preliminarily saturation of nickel at 350-500 C during 5 to 30 min and saturation with boron at 600 to 950 C. The former is conducted in composition containing, wt %: nickel oxide 0.02-0.5, boron carbide 5-35, ammonium chloride 0.005-0.2, sodium tetrafluoroborate 0.01-0.1, and corundum - the balance. EFFECT: enabled preparation of high-quality boron-nickel layers 90-120 mcm thick with microhardness 14000 MPa. 1 tbl |
---|