METHOD OF PREPARING TYPE A ZEOLITE

FIELD: chemical, petroleum, oil refining and gas industries. SUBSTANCE: method comprises calcining kaoline having 53-58 wt % of SiO2 content and 42-47 wt % of Al2O3 content, at temperature of not higher than 850 C for at least 40 minutes, mixing it with alumosilicohydrogel which is mixture of soluti...