METHOD OF PREPARING TYPE A ZEOLITE

FIELD: chemical, petroleum, oil refining and gas industries. SUBSTANCE: method comprises calcining kaoline having 53-58 wt % of SiO2 content and 42-47 wt % of Al2O3 content, at temperature of not higher than 850 C for at least 40 minutes, mixing it with alumosilicohydrogel which is mixture of soluti...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KRYLOV V.O, KOPEIN O.R, TSURIKOV N.K, PANOV D.A, BELOVA O.N
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: chemical, petroleum, oil refining and gas industries. SUBSTANCE: method comprises calcining kaoline having 53-58 wt % of SiO2 content and 42-47 wt % of Al2O3 content, at temperature of not higher than 850 C for at least 40 minutes, mixing it with alumosilicohydrogel which is mixture of solutions of sodium silicates and sodium aluminates, granulation and drying of granules at least three-stage hydrothermal crystallization of granules in alkaline aluminate solution by changing parameters of aluminate solution temperature and granule maintenance time in each crystallization time, washing the zeolite, and squeezing it for 0.5-1.5 h, washing it repeatedly, drying it at temperature of 130-140 C. EFFECT: improved quality of the zeolite. 4 cl