DISPERSEDLY HARDENED COMPOSITION MATERIAL

FIELD: powder metallurgy. SUBSTANCE: proposed composition material comprises, mas. %: aluminium, 0.4-1.0; carbon, 0.15-0.3; oxygen, 0.1-0.2; copper, 98.5-99.35. Hardness of desired material according to Vickers is up to 1910-2000 MPa. Material is wear resistant at elevated temperature. EFFECT: impro...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MATROSOV A.L, DANILOV N.V, KOZITSYN A.A, SHALUNOV E.P, PLEKHANOV K.A
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: powder metallurgy. SUBSTANCE: proposed composition material comprises, mas. %: aluminium, 0.4-1.0; carbon, 0.15-0.3; oxygen, 0.1-0.2; copper, 98.5-99.35. Hardness of desired material according to Vickers is up to 1910-2000 MPa. Material is wear resistant at elevated temperature. EFFECT: improved quality of desired product. 4 dwg , 1 tble