METHOD OF OXIDIZING IRON-CARBON ALLOYS

FIELD: iron alloys. SUBSTANCE: iron-carbon alloys are heated at 600-900 C in mixture containing water vapor and air at weight ratio ranging from 0.02 to 200 (the higher temperature, the larger ratio). EFFECT: increased corrosion resistance of oxide coating of alloys without any technology complicati...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GLINER R.E, CHURAEV V.M, KOLPAKOV A.A, MALEVSKIJ A.K, STAROSTIN V.N, ZHELTOV JU.V, MASLOV V.L, KOSONOGOVA S.A
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: iron alloys. SUBSTANCE: iron-carbon alloys are heated at 600-900 C in mixture containing water vapor and air at weight ratio ranging from 0.02 to 200 (the higher temperature, the larger ratio). EFFECT: increased corrosion resistance of oxide coating of alloys without any technology complication.