FIL BICONSTITUANT POLYOLEFINIQUE ET PROCEDE D'OBTENTION
The process comprises drawing of material consisting of isotactic polypropylene 65-75 and n-dihexylmaleate copolymer 35-25 per cent. Spinning gives a total drawing rate of 1:2.90 - 1:2.95 with reduced material and energy consumption. The creep of the two constituents is 12-16 and 6.5-7.5 g/10 minute...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | fre ; rum |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The process comprises drawing of material consisting of isotactic polypropylene 65-75 and n-dihexylmaleate copolymer 35-25 per cent. Spinning gives a total drawing rate of 1:2.90 - 1:2.95 with reduced material and energy consumption. The creep of the two constituents is 12-16 and 6.5-7.5 g/10 minutes. |
---|