PROCESS FOR PREPARING MALEIC ANHYDRIDE-GRAFTED STYRENE-BUTADIENE BLOCK COPOLYMERS
The invention relates to a process for preparing maleic anhydride-grafted styrene-butadiene block copolymers to be employed as modifiers for crystalline polymers. According to the invention, the process consists in that the maleinization reaction takes place in solution, the reaction medium being an...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rum |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a process for preparing maleic anhydride-grafted styrene-butadiene block copolymers to be employed as modifiers for crystalline polymers. According to the invention, the process consists in that the maleinization reaction takes place in solution, the reaction medium being an ecologically friendly solvent consisting of a mixture of fatty acid methyl esters with 10% butyl acetate, the reaction being performed at a temperature of 75°C for 6 h, at a maleic anhydride/styrene-butadiene block copolymer ratio of 0.075...0.109 and a 2,2'.azo-bis-isobutyronitrile/styrene-butadiene block copolymer ratio of 0.010...0.027.
Invenţia se referă la un procedeu de obţinere a unor bloc-copolimeri stiren butadienici grefaţi cu anhidridă maleică, utilizaţi ca modificatori ai polimerilor cristalini. Procedeul conform invenţiei constă din aceea că reacţia de maleinizare are loc în soluţie utilizând, ca mediu de reacţie, un solvent ecologic constituit dintr-un amestec de esteri metilici ai acizilor graşi cu 10% acetat de butil, reacţia având loc la o temperatură de 75°C, timp de 6 h, la un raport anhidridă maleică/bloc-copolimer stiren butadienic de 0,075...0,109 şi la un raport 2,2'-azo-bis-izobutironitril/bloc-copolimer stiren butadienic de 0,010...0,027. |
---|